PA612 Zytel® 151L DUPONT USA
229
- Properties:Photostabilitylubrication
- Usages:Non specific foodCosmetic
- Certificates:UL
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 1.1 | % | |
TD:3.20mm | 1.1 | % | ||
TD | ISO294-4 | 1.4 | % | |
MD | ISO294-4 | 1.3 | % | |
Moisture Absorption | 饱和,23°C,2.00mm | ISO62 | 3.0 | % |
平衡,23°C,2.00mm,50%RH | ISO62 | 1.3 | % | |
MediumDensity | 0.900 | g/cm³ | ||
SpecificHeatCapacityofMelt | 2750 | J/kg/°C | ||
ThermalConductivityofMelt | 0.18 | W/m/K | ||
Viscosity number | 96%H2SO4 | ISO307 | 95.0 | cm³/g |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | 屈服 | ISO527-2 | 62.0 | Mpa |
Tensile Strain | 屈服 | ISO527-2 | 4.5 | % |
Tensile Modulus | ISO527-2 | 2400 | Mpa | |
Flexural Modulus | ISO178 | 2100 | Mpa | |
Nominal Tensile Strain at Break | ISO527-2 | 17 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Glass Transition Temperature | ISO11357-2 | 65.0 | °C | |
Deflection Temperature Under Load? | 0.45MPa,未退火 | ISO75-2/B | 135 | °C |
1.8MPa,未退火 | ISO75-2/A | 62.0 | °C | |
Linear thermal expansion coefficient | TD:55to160°C | ISO11359-2 | 1.8E-04 | cm/cm/°C |
MD:-- | ISO11359-2 | 1.1E-04 | cm/cm/°C | |
MD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C | |
MD:55to160°C | ISO11359-2 | 1.6E-04 | cm/cm/°C | |
TD:-- | ISO11359-2 | 1.2E-04 | cm/cm/°C | |
TD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C | |
Vicat Softening Temperature | ISO306/B50 | 181 | °C | |
Melting Temperature | ISO11357-3 | 218 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 100Hz | IEC60250 | 0.014 | |
1MHz | IEC60250 | 0.016 | ||
Relative Permittivity | 100Hz | IEC60250 | 3.60 | |
1MHz | IEC60250 | 3.20 | ||
Comparative Tracking Index | IEC60112 | 600 | V | |
Dielectric Strength | IEC60243-1 | 30 | KV/mm | |
Surface Resistivity | IEC60093 | -- | ohms | |
Volume Resistivity | IEC60093 | 1E+15 | ohms·cm |
Film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strain (MD) | Yield | ISO527-3 | 4.5 | % |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | NoBreak | |
23°C | ISO179/1eU | NoBreak |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R级 | ISO2039-2 | 114 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.9mm | UL94 | V-2 | |
1.5mm | UL94 | V-2 | ||
0.9mm | IEC60695-11-10,-20 | V-2 | ||
1.5mm | IEC60695-11-10,-20 | V-2 | ||
Oxygen Index | ISO4589-2 | 27 | % | |
FMVSS Flammability | FMVSS302 | DNI |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
EmissionofOrganicCompounds | VDA277 | 3.10 | µgC/g | |
Odor | VDA270 | 4.50 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.