Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm | | 0.20 | % |
Modeling Shrinkage | TD:3.20mm | | 0.50 | % |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.020 | % |
Density / Specific Gravity | | ASTMD792 | 1.69 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | | ASTMD638 | 179 | Mpa |
Flexural Stress | | ISO178 | 260 | Mpa |
Compressive Strength | | ASTMD695 | 285 | Mpa |
Poisson Ratio | | | 0.39 | |
Tensile Stress | | ISO527-2 | 180 | Mpa |
Tensile Strain | 断裂 | ISO527-2 | 1.4 | % |
Tensile Elongation | 断裂 | ASTMD638 | 1.5 | % |
Flexural Modulus | | ASTMD790 | 14500 | Mpa |
Flexural Modulus | | ISO178 | 14000 | Mpa |
Flexural Strength | | ASTMD790 | 255 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8MPa,未退火 | ASTMD648 | 265 | °C |
Linear thermal expansion coefficient | MD:-50到50°C | ASTME831 | 2E-05 | cm/cm/°C |
Linear thermal expansion coefficient | MD:100到200°C | ASTME831 | 1.5E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:-50到50°C | ASTME831 | 4E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:100到200°C | ASTME831 | 9E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD:导热系数 | ASTME831 | 0.30 | W/m/K |
UL Temperature Rating | | UL746B | 200to220 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
| 90°C | | 1E+11 | ohms |
Comparative Tracking Index | CTI | UL746 | 130 | V |
Dielectric Strength | | ASTMD149 | 22 | KV/mm |
Dissipation Factor? | 25°C,1kHz | ASTMD150 | 2E-03 | |
Dissipation Factor? | 25°C,1MHz | ASTMD150 | 3E-03 | |
Dielectric Constant | 25°C,1kHz | ASTMD150 | 3.80 | |
Dielectric Constant | 25°C,1MHz | ASTMD150 | 3.90 | |
Arc Resistance | | ASTMD495 | 125 | sec |
Volume Resistivity | | ASTMD257 | 1E+16 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod impact strength | | ISO180 | 30 | kJ/m² |
Unnotched Izod Impact Strength | 3.18mm | ASTMD4812 | 510 | J/m |
Notched Izod Impact Strength | 3.17mm | ASTMD256 | 80 | J/m |
Notched Izod Impact Strength | | ISO180/A | 8.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M计秤 | ASTMD785 | 102 | |
Rockwell Hardness | R计秤 | ASTMD785 | 120 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Flame Rating | 1.6mm | UL94 | V-05VA | |
Oxygen Index | | ASTMD2863 | 53 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.