Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced enhance Flame retardant High temperature resistan Filler: Glass fiber reinf 40% filler by weight
- Application Areas:Automotive sector Application in the automo Electrical appliances
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 0.20 | % | |
TD:3.20mm | 0.50 | % | ||
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.020 | % |
Density / Specific Gravity | ASTMD792 | 1.69 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength | ASTMD638 | 179 | Mpa | |
Flexural Stress | ISO178 | 260 | Mpa | |
Compressive Strength | ASTMD695 | 285 | Mpa | |
Poisson Ratio | 0.39 | |||
Tensile Stress | ISO527-2 | 180 | Mpa | |
Tensile Strain | Break | ISO527-2 | 1.4 | % |
Tensile Elongation | Break | ASTMD638 | 1.5 | % |
Flexural Modulus | ASTMD790 | 14500 | Mpa | |
ISO178 | 14000 | Mpa | ||
Flexural Strength | ASTMD790 | 255 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 265 | °C |
Linear thermal expansion coefficient | MD:-50to50°C | ASTME831 | 2E-05 | cm/cm/°C |
MD:100to200°C | ASTME831 | 1.5E-05 | cm/cm/°C | |
TD:-50to50°C | ASTME831 | 4E-05 | cm/cm/°C | |
TD:100to200°C | ASTME831 | 9E-05 | cm/cm/°C | |
TD:导热系数 | ASTME831 | 0.30 | W/m/K | |
UL Temperature Rating | UL746B | 200to220 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
InsulationResistance2 | 90°C | 1E+11 | ohms | |
Comparative Tracking Index | CTI | UL746 | 130 | V |
Dielectric Strength | ASTMD149 | 22 | KV/mm | |
Dissipation Factor? | 25°C,1kHz | ASTMD150 | 2E-03 | |
25°C,1MHz | ASTMD150 | 3E-03 | ||
Dielectric Constant | 25°C,1kHz | ASTMD150 | 3.80 | |
25°C,1MHz | ASTMD150 | 3.90 | ||
Arc Resistance | ASTMD495 | 125 | sec | |
Volume Resistivity | ASTMD257 | 1E+16 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod impact strength | ISO180 | 30 | kJ/m² | |
Unnotched Izod Impact Strength | 3.18mm | ASTMD4812 | 510 | J/m |
Notched Izod Impact Strength | 3.17mm | ASTMD256 | 80 | J/m |
ISO180/A | 8.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Sale | ASTMD785 | 102 | |
R-Sale | ASTMD785 | 120 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flame Rating | 1.6mm | UL94 | V-05VA | |
Oxygen Index | ASTMD2863 | 53 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.