physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | TD | ISO294-4 | 1.4 | % |
MD | ISO294-4 | 1.4 | % | |
Water absorption rate | 23°C,24hr | ISO62 | 0.60 | % |
饱和,23°C,2.00mm | ISO62 | 0.60 | % | |
平衡,23°C,2.00mm,50%RH | ISO62 | 0.20 | % | |
Melt mass flow rate | ISO1133 | 18 | g/10min | |
MediumDensity | 1.04 | g/cm³ | ||
SpecificHeatCapacity of Melt | 2110 | J/kg/°C | ||
ThermalConductivityofMelt | 0.19 | W/m/K | ||
Melt volume flow rate | 220°C/2.16kg | ISO1133 | 17.5 | cm3/10min |
Density/specific gravity | ISO1183 | 1.19 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Nominal tensile fracture strain | ISO527-2 | 780 | % | |
abrasion resistance | ISO4649 | 120 | mm³ | |
Tensile creep modulus | 1000hr | ISO899-1 | 130 | Mpa |
TensileCreepModule | 1hr | ISO899-1 | 170 | Mpa |
Tensile stress | 屈服 | ISO527-2 | 15.0 | Mpa |
断裂 | ISO527-2 | 40.0 | Mpa | |
5.0%应变 | ISO527-2 | 6.90 | Mpa | |
10%应变 | ISO527-2 | 11.0 | Mpa | |
50%应变 | ISO527-2 | 14.0 | Mpa | |
Tensile strain | 屈服 | ISO527-2 | 35 | % |
断裂 | ISO527-2 | >300 | % | |
Tensile modulus | ISO527-2 | 190 | Mpa | |
Bending modulus | ISO178 | 200 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,未退火 | ISO75-2/B | 65.0 | °C |
1.8MPa,未退火 | ISO75-2/A | 45.0 | °C | |
Brittle temperature | ISO974 | -98.0 | °C | |
Vicat softening temperature | -- | ISO306/A50 | 180 | °C |
-- | ISO306/B50 | 75.0 | °C | |
Glass transition temperature 2 | ISO11357-2 | -20.0 | °C | |
Melting temperature 2 | ISO11357-3 | 203 | °C | |
Linear coefficient of thermal expansion | MD:-- | ISO11359-2 | 2E-04 | cm/cm/°C |
MD:-40to23°C | ISO11359-2 | 1.8E-04 | cm/cm/°C | |
TD:-- | ISO11359-2 | 2E-04 | cm/cm/°C | |
TD:-40to23°C | ISO11359-2 | 1.7E-04 | cm/cm/°C | |
TD:EffectiveThermalDiffusivity | ISO11359-2 | 9E-08 | m²/s |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric strength | IEC60243-1 | 20 | KV/mm | |
Dissipation factor | 1MHz | IEC60250 | 0.038 | |
100Hz | IEC60250 | 9E-03 | ||
Relative permittivity | 1MHz | IEC60250 | 4.60 | |
100Hz | IEC60250 | 4.90 | ||
Leakage Trace Index | IEC60112 | 600 | V | |
Surface resistivity | IEC60093 | >1.0E+15 | ohms | |
Volume resistivity | IEC60093 | 4E+13 | ohms·cm |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
tear strength | 横向流量 | ISO34-1 | 130 | kN/m |
流量 | ISO34-1 | 130 | kN/m |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -40°C | ISO179/1eA | 30 | kJ/m² |
-30°C,局部断裂 | ISO179/1eA | 150 | kJ/m² | |
23°C | ISO179/1eA | NoBreak | ||
Tensile impact strength | 23°C | ISO8256/1 | 270 | kJ/m² |
Impact strength of simply supported beam without notch | -30°C | ISO179/1eU | NoBreak | |
23°C | ISO179/1eU | NoBreak |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | 邵氏D | ISO868 | 55 | |
邵氏D,15秒 | ISO868 | 51 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 3.0mm | IEC60695-11-10,-20 | HB | |
1.5mm | IEC60695-11-10,-20 | HB | ||
3.0mm | UL94 | HB | ||
1.5mm | UL94 | HB | ||
Extreme Oxygen Index | ISO4589-2 | 21 | % | |
FMVSS flammability | FMVSS302 | SE/B | ||
Fogging-G-value | condensate | ISO6452 | 1E-04 | g |
Burning rate 3 | 1.00mm | ISO3795 | 28 | mm/min |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Odor | VDA270 | 5.00 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.