PPO FLEX NORYL™ WCD931 BK1006 SABIC INNOVATIVE JAPAN
70
- Unit Price:
- $469 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 12.3MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High impact resistance transparent
- Application Areas:Automotive interior parts
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 250°C/10.0kg | ASTMD1238 | 8.5 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength | Break | CCP METHOD | 15.0 | Mpa |
Break2 | ASTMD638 | 9.00 | Mpa | |
Break,80°C3 | CCP METHOD | 15.0 | Mpa | |
Tensile stress | Break | ISO527-2/50 | 9.00 | Mpa |
elongation | Break | CCP METHOD | 310 | % |
Break2 | ASTMD638 | 130 | % | |
Break,80°C3 | CCP METHOD | 270 | % | |
Tensile strain | Break | ISO527-2/50 | 180 | % |
Bending modulus 4 | 100mmSpan | ASTMD790 | 160 | Mpa |
ISO178 | 135 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Brittle temperature | ASTMD746 | <-40.0 | °C | |
HeatDeformation5 | 100°C | CCP METHOD | 10 | % |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume resistivity | ASTMD257 | 2E+15 | ohms·cm | |
Electrical strength | 2.00mm,inOil | IEC60243-1 | 23 | KV/mm |
Dielectric constant | 1MHz | ASTMD150 | 3.00 | |
Dissipation factor | 1MHz | ASTMD150 | 1E-03 | |
Leakage Trace Index | IEC60112 | 600 | V |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A,30sec | ASTMD2240 | 93 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning wire flammability index | 3.0mm | IEC60695-2-12 | 750 | °C |
Hot filament ignition temperature | 3.0mm | IEC60695-2-13 | 775 | °C |
Extreme Oxygen Index | ISO4589-2 | 29 | % | |
Smoke density | Flame,0.5mmplaque,Ds,max | ASTME662 | 56 | |
Non-Flame,0.5mmplaque,Ds,max | ASTME662 | 150 | ||
VerticalFlameTest | EN50265-2-1 | PASSES |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.