PC/PTFE LNP™ LUBRICOMP™ DFL-4034 SABIC INNOVATIVE US
225
- Unit Price:
- $8100 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 21MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Easy to form Easy to demould
- Application Areas:Electronic and Electrical Lighting applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:24hr | ASTMD955 | 0.020到0.040 | % |
TD:24hr | ASTMD955 | 0.20到0.40 | % | |
24hr,50%RH | ASTMD570 | 0.090 | % | |
Balance, 23 ° C, 50% RH | ISO62 | 0.13 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
--1 | ASTMD638 | 7190 | Mpa | |
Fracture 2 | ASTMD638 | 95.0 | Mpa | |
crack | ISO527-2/5 | 93.0 | Mpa | |
Wear factor | Washer | ASTMD3702Modified | 89.0 | 10^-10in^5-min/ft-lb-hr |
yield | ISO527-2/5 | 2.8 | % | |
Fracture 3 | ASTMD638 | 2.7 | % | |
crack | ISO527-2/5 | 3.1 | % | |
50.0mm span 4 | ASTMD790 | 6320 | Mpa | |
--5 | ISO178 | 6200 | Mpa | |
Fracture, 50.0mm span 6 | ASTMD790 | 145 | Mpa | |
friction coefficient | Itself - Dynamic | ASTMD3702Modified | 0.46 | |
Itself - Static | ASTMD3702Modified | 0.50 | ||
Wear factor | Ring | ASTMD3702Modified | 13.0 | 10^-10in^5-min/ft-lb-hr |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
0.45MPa, unannealed, 3.20mm | ASTMD648 | 146 | °C | |
0.45MPa, unannealed, 64.0mm span 9 | ISO75-2/Bf | 146 | °C | |
1.8MPa, unannealed, 3.20mm | ASTMD648 | 142 | °C | |
1.8MPa, unannealed, 64.0mm span of 10 | ISO75-2/Af | 141 | °C | |
Linear coefficient of thermal expansion | MD:-30to30°C | ASTMD696 | 3.7E-05 | cm/cm/°C |
TD:-30to30°C | ASTMD696 | 6.3E-05 | cm/cm/°C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
23°C | ASTMD256 | 150 | J/m | |
23°C7 | ISO180/1A | 14 | kJ/m² | |
23°C | ASTMD4812 | 740 | J/m | |
23°C8 | ISO180/1U | 49 | kJ/m² | |
23°C,TotalEnergy | ASTMD3763 | 19.6 | J | |
-- | ISO6603-2 | 6.60 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.