Need Help? Contact Us service@plas.com
Get App

TPV X4765B DSM HOLAND

128
  • Unit Price:
    $3258 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:--
  • Application Areas:--
  • Color:--
  • Grade:Extrusion grade

Technical Data Sheet Compare

ageingTest ConditionTest MethodTest ResultUnit
Change rate of tensile strength in air - transverse flow rate135°C,1000hrASTMD573-18%
Change rate of tensile strength in air - transverse flow rate135°C,1000hrISO188-18%
Change rate of tensile strength in air - transverse flow rate100%Strain135°C,1000hrASTMD5731.0%
Change rate of tensile strength in air - transverse flow rate100%Strain135°C,1000hrISO1881.0%
Change rate of tensile strength in air - transverse flow rate150°C,168hrASTMD573-20%
Change rate of tensile strength in air - transverse flow rate150°C,168hrISO188-20%
Change rate of tensile strength in air - transverse flow rate100%Strain150°C,168hrASTMD5730.0%
Change rate of tensile strength in air - transverse flow rate100%Strain150°C,168hrISO1880.0%
Tensile stress variation during fracture in air - transverse flow rate135°C,1000hrASTMD573-22%
Tensile stress variation during fracture in air - transverse flow rate135°C,1000hrISO188-22%
Tensile stress variation during fracture in air - transverse flow rate150°C,168hrASTMD573-24%
Tensile stress variation during fracture in air - transverse flow rate150°C,168hrISO188-24%
Change rate of Shore hardness in airShore A,135°C,1000hrASTMD5731.0
Change rate of Shore hardness in airShore A,135°C,1000hrISO1881.0
Change rate of Shore hardness in airShore A,150°C,168hrASTMD5731.0
Change rate of Shore hardness in airShore A,150°C,168hrISO1881.0
Volume change135°C,70hr,inIRM903OilISO181784%
Volume change135°C,70hr,inIRM903OilASTMD47184%
elastomerTest ConditionTest MethodTest ResultUnit
Tensile stress流量:BreakASTMD4124.90Mpa
Tensile stress流量:BreakISO374.90Mpa
elongationBreakASTMD412400%
elongationBreakISO37400%
elongation流量:BreakASTMD412340%
elongation流量:BreakISO37340%
Tear strength - transverse flow rate--ASTMD62425kN/m
Tear strength - transverse flow rate--2ISO34-125kN/m
Permanent compression deformation23°C,22hrASTMD39523%
Permanent compression deformation23°C,22hrISO81523%
Tensile stressAcross Flow:100%StrainASTMD4122.30Mpa
Tensile stressAcross Flow:100%StrainISO372.30Mpa
Tensile stress流量:100%StrainASTMD4122.90Mpa
Tensile stress流量:100%StrainISO372.90Mpa
Tensile stressBreakASTMD4125.10Mpa
Tensile stressBreakISO375.10Mpa
Permanent compression deformation70°C,22hrASTMD39532%
Permanent compression deformation70°C,22hrISO81532%
Permanent compression deformation125°C,70hrASTMD39548%
Permanent compression deformation125°C,70hrISO81548%
hardnessTest ConditionTest MethodTest ResultUnit
Shore hardnessShore A,5sec,挤塑ASTMD224062
Shore hardnessShore A,5sec,挤塑ISO86862
Shore hardnessShore A,5sec,InjectionASTMD224065
Shore hardnessShore A,5sec,InjectionISO86865
Supplementary InformationTest ConditionTest MethodTest ResultUnit
ApparentShearViscosity-Capillary,@206/s200°CASTMD3835210Pa·s
ApparentShearViscosity-Capillary,@206/s200°CISO11443210Pa·s
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.