Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPV X4765B DSM HOLAND
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
ageing
Test Condition
Test Method
Unit
TPV/DSM HOLAND/X4765B
Change rate of tensile strength in air - transverse flow rate
135°C,1000hr
ASTMD573
%
-
Change rate of tensile strength in air - transverse flow rate
135°C,1000hr
ISO188
%
-
Change rate of tensile strength in air - transverse flow rate
100%应变135°C,1000hr
ASTMD573
%
1
Change rate of tensile strength in air - transverse flow rate
100%应变135°C,1000hr
ISO188
%
1
Change rate of tensile strength in air - transverse flow rate
150°C,168hr
ASTMD573
%
-
Change rate of tensile strength in air - transverse flow rate
150°C,168hr
ISO188
%
-
Change rate of tensile strength in air - transverse flow rate
100%应变150°C,168hr
ASTMD573
%
0
Change rate of tensile strength in air - transverse flow rate
100%应变150°C,168hr
ISO188
%
0
Volume change
135°C,70hr,inIRM903Oil
ISO1817
%
8
Volume change
135°C,70hr,inIRM903Oil
ASTMD471
%
8
Tensile stress variation during fracture in air - transverse flow rate
135°C,1000hr
ASTMD573
%
-
Tensile stress variation during fracture in air - transverse flow rate
135°C,1000hr
ISO188
%
-
Tensile stress variation during fracture in air - transverse flow rate
150°C,168hr
ASTMD573
%
-
Tensile stress variation during fracture in air - transverse flow rate
150°C,168hr
ISO188
%
-
elastomer
Test Condition
Test Method
Unit
TPV/DSM HOLAND/X4765B
Tensile stress
流量:断裂
ASTMD412
Mpa
4
Tensile stress
流量:断裂
ISO37
Mpa
4
Tensile stress
横向流量:100%应变
ASTMD412
Mpa
2
Tensile stress
横向流量:100%应变
ISO37
Mpa
2
Tensile stress
流量:100%应变
ASTMD412
Mpa
2
Tensile stress
流量:100%应变
ISO37
Mpa
2
Tensile stress
断裂
ASTMD412
Mpa
5
Tensile stress
断裂
ISO37
Mpa
5
elongation
断裂
ASTMD412
%
4
elongation
断裂
ISO37
%
4
elongation
流量:断裂
ASTMD412
%
3
elongation
流量:断裂
ISO37
%
3
Tear strength - transverse flow rate
--
ASTMD624
kN/m
2
Tear strength - transverse flow rate
--2
ISO34-1
kN/m
2
Permanent compression deformation
23°C,22hr
ASTMD395
%
2
Permanent compression deformation
23°C,22hr
ISO815
%
2
Permanent compression deformation
70°C,22hr
ASTMD395
%
3
Permanent compression deformation
70°C,22hr
ISO815
%
3
Permanent compression deformation
125°C,70hr
ASTMD395
%
4
Permanent compression deformation
125°C,70hr
ISO815
%
4
Supplementary Information
Test Condition
Test Method
Unit
TPV/DSM HOLAND/X4765B
ApparentShearViscosity-Capillary,@206/s
200°C
ASTMD3835
Pa·s
2
ApparentShearViscosity-Capillary,@206/s
200°C
ISO11443
Pa·s
2