Need Help? Contact Us service@plas.com
Get App

PEI LNP™ STAT-KON™  EX99689C SABIC INNOVATIVE US

112
  • Unit Price:
    $10873 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Glass fiber reinforced lubrication
  • Application Areas:Electrical and Electronic Automotive components
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9550.20%
Shrinkage rateTD:24hrASTMD9550.40%
Shrinkage rateTD:24hrISO294-40.36%
Shrinkage rateMD:24hrISO294-40.17%
Water absorption rate24hr,50%RHASTMD5700.30%
Water absorption rateEquilibrium,23°C,50%RHISO620.35%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulus 2ASTMD63811700Mpa
Tensile modulusISO527-2/112600Mpa
Tensile strengthBreakASTMD638161Mpa
Tensile stressBreakISO527-2137Mpa
elongationBreakASTMD6381.6%
Tensile strainBreakISO527-21.2%
Bending modulus 450.0mmSpanASTMD7908000Mpa
Bending modulus 4ISO1787700Mpa
bending strength ASTMD790242Mpa
Bending stressISO178216Mpa
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD648206°C
Hot deformation temperature 61.8MPa,Unannealed,64.0mmSpanISO75-2/Af207°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8313.3E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CISO11359-23.3E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CASTME8313.3E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CISO11359-23.3E-05cm/cm/°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Surface resistivityASTMD2571.0E+2to1.0E+6ohms
Impact performanceTest ConditionTest MethodTest ResultUnit
Suspended wall beam gap impact strength 523°CISO180/1A5.1kJ/m²
Unscented Izod Impact Strength 523°CISO180/1U28kJ/m²
Dart impact equipped with measuring instruments23°C,EnergyatPeakLoadASTMD376311.4J
Multi axis Instrumented Impact EnergyISO6603-22.41J
flammabilityTest ConditionTest MethodTest ResultUnit
FlameRating0.35mm,TestingbySABICUL94V-0
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.