PEI ULTEM™ AUT195 BK1343M SABIC INNOVATIVE US
106
- Unit Price:
- $16395 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 16MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility High transparency high definition
- Application Areas:Electrical appliances Automotive Applications
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | TD2 | 内部方法 | 0.50to0.70 | % |
MD:3.20mm | 内部方法 | 0.50to0.70 | % | |
Water absorption rate | Saturation,23°C | ISO62 | 0.90 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.50 | % | |
Melt mass flow rate | 337°C/6.6kg | ASTMD1238 | 24 | g/10min |
Melt volume flow rate | 340°C/5.0kg | ISO1133 | 16.0 | cm3/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2/1 | 3000 | Mpa | |
Tensile strength 3 | Yield | ASTMD638 | 96.5 | Mpa |
Bending modulus 4 | 100mmSpan | ASTMD790 | 3170 | Mpa |
Elongation rate 4 | Break | ASTMD638 | 70 | % |
Bending modulus 5 | ISO178 | 3100 | Mpa | |
Flexural Strength4 | Yield,100mmSpan | ASTMD790 | 145 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature 8 | 1.8MPa,Unannealed,100mmSpan | ISO75-2/Ae | 180 | °C |
0.45MPa,Unannealed,100mmSpan | ISO75-2/Be | 195 | °C | |
Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 190 | °C |
Vicat softening temperature | ISO306/B120 | 205 | °C | |
thermal conductivity | ISO8302 | 0.23 | W/m/K | |
Linear coefficient of thermal expansion | MD:23to150°C | ISO11359-2 | 6E-05 | cm/cm/°C |
TD:23to150°C | ISO11359-2 | 6E-05 | cm/cm/°C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Suspended wall beam gap impact strength 7 | -30°C | ISO180/1A | 5.0 | kJ/m² |
23°C | ISO180/1A | 5.0 | kJ/m² | |
Impact strength of simply supported beam gap 6 | 23°C | ISO179/1eA | 4.0 | kJ/m² |
-30°C | ISO179/1eA | 4.0 | kJ/m² | |
ReverseNotchIzodImpact | 3.20mm | ASTMD256 | 2100 | J/m |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
MetallizedHazeOnset | 内部方法 | 195 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.