Technical Data Sheet
Compare
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Melt mass flow rate | 315°C/5.0kg | ASTMD1238 | 90 | g/10min |
Shrinkage rate | MD | 内部方法 | 0.30 | % |
Shrinkage rate | TD | 内部方法 | 0.60 | % |
Water absorption rate | Equilibrium | ASTMD570 | >0.020 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | | ASTM D-785 | 121 | |
tensile strength | | ASTM D-638 | 123 | Mpa |
bending strength | | ASTM D-790 | 225 | Mpa |
Bending modulus | | ASTM D-790 | 20 | GPa |
Charpy impact strength | 有Notched | ASTM D-256 | 64 | J/m |
Charpy impact strength | Unnotched | ASTM D-256 | 206 | J/m |
Elongation rate | | ASTM D-638 | 0.8 | % |
Tensile strength | | ASTMD638 | 116 | Mpa |
elongation | Break | ASTMD638 | 0.60 | % |
Bending modulus | | ASTMD790 | 20000 | Mpa |
bending strength | | ASTMD790 | 221 | Mpa |
Tensile Weld Strength | | ASTMD638 | 39.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Linear coefficient of thermal expansion | | 自定标准 | 2 | |
Flame retardancy | | UL 94 | V-0 | |
Hot deformation temperature | 1.82MPa | ASTM D-648 | >260 | °C |
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | >260 | °C |
Melting temperature | | 内部方法 | 285 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | | ASTMD257 | 1E+18 | ohms·cm |
Dielectric strength | | ASTMD149 | 15 | KV/mm |
Dielectric constant | 1MHz | ASTMD150 | 4.90 | |
Dissipation factor | 1MHz | ASTMD150 | 1.5E-03 | |
Arc resistance | | ASTMD495 | 150 | sec |
Dielectric breakdown strength | | ASTM D-149 | 14 | KV/mm |
Volume resistance value | | ASTM D-257 | 4×1016 | Ω.cm |
Dielectric constant | 1MHz | ASTM D-150 | 4.9 | |
Dissipation coefficient | 1MHz | ASTM D-150 | 0.0015 | |
Thermal conductivity | | 自定标准 | 0.48 | W/m.K |
Processing performance | Test Condition | Test Method | Test Result | Unit |
---|
Shrinkage rate | Flow | ASTM D-955 | 0.3 | % |
Shrinkage rate | Across Flow | ASTM D-955 | 0.6 | % |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Cantilever beam without notch impact strength | | ASTMD256 | 210 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | R-Scale | ASTMD785 | 121 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | | UL94 | V-0 | |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|
density | | ASTM D-792 | 1.94 | |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|
BarFlowLength | 1.00mm | 内部方法 | 125 | mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.