Technical Data Sheet
Compare
physical property | Test Condition | Test Method | Test Result | Unit |
---|
MediumDensity | | | 1.20 | g/cm³ |
Melt mass flow rate | | ISO1133 | 14 | g/10min |
Melt volume flow rate | 190°C/2.16kg | ISO1133 | 12.0 | cm3/10min |
Shrinkage rate | TD | ISO294-4 | 1.8 | % |
Shrinkage rate | MD | ISO294-4 | 2.0 | % |
Water absorption rate | Saturation,23°C,2.00mm | ISO62 | 0.90 | % |
Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO62 | 0.20 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile modulus | | ISO527-2 | 3350 | Mpa |
Tensile stress | Yield | ISO527-2 | 73.5 | Mpa |
Tensile strain | Yield | ISO527-2 | 13 | % |
Nominal tensile fracture strain | | ISO527-2 | 27 | % |
Bending modulus | | ISO178 | 3150 | Mpa |
Bending stress | 3.5%Strain | ISO178 | 85.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 159 | °C |
Hot deformation temperature | 1.8MPa,Unannealed | ISO75-2/A | 103 | °C |
Melting temperature 2 | | ISO11357-3 | 178 | °C |
Linear coefficient of thermal expansion | MD:-- | ISO11359-2 | 1E-04 | cm/cm/°C |
Linear coefficient of thermal expansion | MD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | TD:-- | ISO11359-2 | 1E-04 | cm/cm/°C |
Linear coefficient of thermal expansion | TD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | TD:AnnealingTemperature | ISO11359-2 | 160 | °C |
Linear coefficient of thermal expansion | TD:AnnealingTime-Optional | ISO11359-2 | 30.0 | min/mm |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface resistivity | | IEC60093 | >1.0E+15 | ohms |
Volume resistivity | | IEC60093 | >1.0E+15 | ohms·cm |
Dielectric strength | | IEC60243-1 | 43 | KV/mm |
Relative permittivity | 100Hz | IEC60250 | 3.90 | |
Relative permittivity | 1MHz | IEC60250 | 3.80 | |
Dissipation factor | 100Hz | IEC60250 | 5E-04 | |
Dissipation factor | 1MHz | IEC60250 | 5.5E-03 | |
Leakage Trace Index | | IEC60112 | 600 | V |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Impact strength of simply supported beam without notch | -30°C | ISO179/1eU | 230 | kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO179/1eU | 250 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | M-Sale | ISO2039-2 | 93 | |
Rockwell hardness | R-Sale | ISO2039-2 | 121 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
Burning rate 3 | 1.00mm | ISO3795 | <100 | mm/min |
FMVSS flammability | | FMVSS302 | B | |
Fogging-G-value | condensate | ISO6452 | 3.5E-04 | g |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|
Emission | | VDA275 | <2.00 | mg/kg |
EmissionofOrganicCompounds | | VDA277 | 10.0 | µgC/g |
Odor | | VDA270 | 3.50 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.