PA6 Zytel® 73G45L DUPONT USA
127
- Unit Price:
- $3728 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability Filler: Glass fiber reinf 45% filler by weight
- Application Areas:Electronic and electrical Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ISO1183 | 1.51 | g/cm³ | |
Shrinkage rate | TD | ISO294-4 | 0.90 | % |
MD | ISO294-4 | 0.10 | % | |
Water absorption rate | Saturation,23°C,2.00mm | ISO62 | 4.9 | % |
Equilibrium,23°C,2.00mm,50%RH | ISO62 | 1.5 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2 | 14500 | Mpa | |
Tensile stress | Break | ISO527-2 | 230 | Mpa |
Tensile strain | Break | ISO527-2 | 3.0 | % |
TensileCreepModule | 1hr | ISO899-1 | -- | Mpa |
Tensile creep modulus | 1000hr | ISO899-1 | -- | Mpa |
Bending modulus | ISO178 | 13000 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 221 | °C |
1.8MPa,Unannealed | ISO75-2/A | 213 | °C | |
Vicat softening temperature | ISO306/B50 | 215 | °C | |
Melting temperature 2 | ISO11357-3 | 221 | °C | |
Linear coefficient of thermal expansion | MD | ISO11359-2 | 1.6E-05 | cm/cm/°C |
TD | ISO11359-2 | 1E-04 | cm/cm/°C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 19 | kJ/m² |
23°C | ISO179/1eA | 20 | kJ/m² | |
Impact strength of simply supported beam without notch | -30°C | ISO179/1eU | 120 | kJ/m² |
23°C | ISO179/1eU | 120 | kJ/m² | |
Impact strength of cantilever beam gap | -30°C | ISO180/1A | 15 | kJ/m² |
23°C | ISO180/1A | 18 | kJ/m² |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning rate 3 | 1.00mm | ISO3795 | 44 | mm/min |
UL flame retardant rating | 1.5mm | UL94 | HB | |
Flammability level | 1.5mm | IEC60695-11-10,-20 | HB | |
FMVSS flammability | FMVSS302 | B |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.