Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | 24hr | ASTMD570 | 7E-03 | % |
Melt Mass-Flow Rate | 297°C/5.0kg | ASTMD3159 | 6.0 | g/10min |
Apparent Density | | 内部方法 | 1.30 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Compressive Strength | 23°C | ASTMD695 | 17.0 | Mpa |
Tensile Strength | 23°C | ASTMD638 | 40.0 | Mpa |
Tensile Elongation | 断裂,23°C | ASTMD638 | 300 | % |
Flexural Modulus | 23°C | ASTMD790 | 1000 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Linear thermal expansion coefficient | MD:0到100°C | ASTMD696 | 1.3E-04 | cm/cm/°C |
Melting temperature | | ASTMD3418 | 255to280 | °C |
Maximum Service Temperature | | UL746 | 155 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | 0.250mm | ASTMD149 | 70 | KV/mm |
Dissipation Factor? | 23°C,1MHz | ASTMD1531 | 6E-03 | |
Dielectric Constant | 23°C,1MHz | ASTMD1531 | 2.50to2.60 | |
Arc Resistance | | ASTMD495 | 122 | sec |
Volume Resistivity | | ASTMD257 | 1E+17 | ohms·cm |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | 邵氏D | ASTMD2240 | 67 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | | UL94 | V-0 | |
Oxygen Index | | ASTMD2863 | 30to32 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.