Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Content | | | < 0.020 | % |
Modeling Shrinkage - Flow | 3.20 mm | ASTM D955 | 0.60 到 0.80 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | | ASTM D638 | 58.6 | Mpa |
Tensile Modulus | | ASTM D638 | 2140 | Mpa |
Tensile Elongation | 屈服 | ASTM D638 | 8.0 | % |
Flexural Modulus | | ASTM D790 | 2280 | Mpa |
Flexural Strength | | ASTM D790 | 82.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8 MPa, 未退火 | ASTM D648 | 64.4 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
| | FTMS 101C 4046.1 | < 2.0 | sec |
Surface Resistivity | -- | ESD STM11.11 | 1.0E+5 到 1.0E+9 | ohms |
Surface Resistivity | -- | ASTM D257 | 1.0E+6 到 1.0E+10 | ohms |
Volume Resistivity | | ASTM D257 | 1.0E+2 到 1.0E+5 | ohms·cm |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Drying Temperature | | | 79 | °C |
Processing (Melt) Temp | | | 232 到 282 | °C |
Mold Temperature | | | 49 到 93 | °C |
Drying Time | | | 4.0 | hr |
Injection Pressure | | | 68.9 到 103 | Mpa |
| | | -40 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Unnotched Izod Impact Strength | 3.20 mm | ASTM D4812 | 无断裂 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.