Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | 300℃,1.2kg | ASTM D-1238(ISO 1133) | 25 | g/10min |
Modeling Shrinkage | 23℃ | Internal Method | 0.5-0.7 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Unnotched Izod Impact Strength | 23℃,3.18mm | ASTM D-256 | 640 | J/m |
Rockwell Hardness | 23℃ | ASTM D-785(ISO 2039/2) | 122 | |
Flexural Modulus | 23℃ | ASTM D-790(ISO 178) | 2250 | Mpa |
Flexural Strength | 23℃ | ASTM D-790(ISO 178) | 98 | Mpa |
Tensile Strength | 屈服,23℃ | ASTM D-638(ISO 527-2) | 59 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8MPa,未退水,3.18mm | ASTM D-648 | 110 | °C |
Deflection Temperature Under Load? | 热变形温度,1.8MPa,未退水,3.18mm跨距 | ISO 75-2/A | 110 | °C |
Deflection Temperature Under Load? | Test Condition | Test Method | Test Result | Unit |
---|
Flammability | 阻燃等级,1.5mm | UL 94 | V0 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.