Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Apparent Density | | ASTMD4894 | 0.36 | g/cm³ |
Modeling Shrinkage | MD | 内部方法 | 4.4 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | 屈服,1.50mm | ASTMD4894 | 40.0 | Mpa |
Compressive Strength | 0%应变2 | ASTMD695 | 8.70 | Mpa |
Compressive Strength | 1%应变3 | ASTMD695 | 5.90 | Mpa |
Compressive Strength | 25%应变3 | ASTMD695 | 28.6 | Mpa |
Heat Deflection Temperature | 25°C,14MPa | ASTMD621 | 10.6 | % |
Heat Deflection Temperature | 100°C,14MPa | ASTMD621 | 21.7 | % |
Heat Deflection Temperature | 200°C,6.9MPa | ASTMD621 | 14.9 | % |
Tensile Elongation | 断裂,1.50mm | ASTMD4894 | 500 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melting temperature | | DSC | 324 | °C |
Continuous Use Temperature | | | 260 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | | | 140 | KV/mm |
Surface Resistivity | | ASTMD257 | >1.0E+15 | ohms |
Dielectric Constant | 1kHz | ASTMD150 | <2.10 | |
Volume Resistivity | | ASTMD257 | >1.0E+18 | ohms·cm |
Dissipation Factor? | 1kHz | ASTMD150 | <1.0E-4 | |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|
Compression Set | 25°C4 | ASTMD621 | 3.0 | % |
Compression Set | 100°C4 | ASTMD621 | 7.4 | % |
Compression Set | 200°C5 | ASTMD621 | 4.1 | % |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|
| | ASTMD2178 | 3E+06 | |
| | ASTMD4895 | 62.0 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.