Modeling Shrinkage | MD | ASTMD955 | 0.60 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Stress | 23°C | ISO178 | 60.0 | Mpa |
Flexural Stress | 屈服,23°C | ASTMD790 | 64.0 | Mpa |
Tensile Modulus | 23°C | ASTMD638 | 1610 | Mpa |
Tensile Modulus | 23°C | ISO527-2 | 1570 | Mpa |
Tensile Elongation | 屈服,23°C | ASTMD638,ISO527-2 | 7.0 | % |
Tensile Elongation | 断裂,23°C | ASTMD638,ISO527-2 | 140 | % |
Flexural Modulus | 23°C | ASTMD790 | 1520 | Mpa |
Flexural Modulus | 23°C | ISO178 | 1490 | Mpa |
Tensile Strength | 屈服,23°C | ASTMD638,ISO527-2 | 45.0 | Mpa |
Tensile Strength | 断裂,23°C | ASTMD638 | 52.0 | Mpa |
Tensile Strength | 断裂,23°C | ISO527-2 | 51.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,未退火 | ASTMD648 | 101 | °C |
Deflection Temperature Under Load? | 1.8MPa,未退火 | ASTMD648 | 85.0 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 无断裂 | |
Instrumented Dart Impact | -40°C,EnergyatPeakLoad | ASTMD3763 | 67.0 | J |
Instrumented Dart Impact | 0°C,EnergyatPeakLoad | ASTMD3763 | 65.0 | J |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 62.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R级,23°C | ASTMD785 | 110 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Haze | | ASTMD1003 | <1.0 | % |
Transmittance | 总计 | ASTMD1003 | 91.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.