Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Shrinkage rate | MD:2.00mm | ASTMD955 | 1.8 | % |
Shrinkage rate | TD:2.00mm | ASTMD955 | 1.5 | % |
Water absorption rate | 24hr | ASTMD570 | 0.010 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Bending modulus 3 | 23°C,3.00mm,48.0mmSpan | ASTMD790 | 1590 | Mpa |
Tensile strength 2 | 断裂,23°C | ASTMD638 | 41.0 | Mpa |
Elongation rate 2 | 断裂,23°C | ASTMD638 | 12 | % |
FlexuralStrength3 | Yield,23°C,3.00mm,48.0mmSpan | ASTMD790 | 37.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Vicat softening temperature | | ASTMD15254 | 130 | °C |
Hot deformation temperature | 0.45MPa,未退火 | ASTMD648 | 80.0 | °C |
Linear coefficient of thermal expansion | MD | ASTMD696 | 1.3E-04 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric strength | | ASTMD149 | 45 | KV/mm |
Dielectric constant | 23°C | ASTMD150 | 2.30 | |
Volume resistivity | | ASTMD257 | 1E+17 | ohms·cm |
Dissipation factor | 1MHz | ASTMD150 | 1.5E-04 | |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
NotchedIzodImpact | 23°C,2.00mm | ASTMD256 | 190 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | R级 | ASTMD785 | 53 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
FlameRating | 1.6mm | UL94 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.