189
- Properties:Glass fiber reinforceddimensional stabilityHigh rigidityhigh strengthheat-resisting
- Usages:Lawn equipmentElectrical fieldElectrical appliancesElectronic fieldElectronic displayEngine hood partsTextile applicationIndustrial applicationsNursing suppliesHousehold goodsArchitectural applicationAutomotive interior partsAutomotive External PartsPetroleum ApplicationsOutdoor applicationssporting goodsNatural gas suppliesMedical suppliesGarden equipmentLighting fixturesLighting applications
- Certificates:UL
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:--3 | 内部方法 | 0.30to0.50 | % |
TD:3.20mm | 内部方法 | 0.50to1.0 | % | |
TD:--2 | 内部方法 | 0.50to1.0 | % | |
TD:--5 | 内部方法 | 0.60to0.90 | % | |
TD:--3 | 内部方法 | 0.40to0.60 | % | |
MD:--4 | 内部方法 | 0.50to0.80 | % | |
MD:--2 | 内部方法 | 0.30to0.70 | % | |
MD:3.20mm | 内部方法 | 0.30to0.80 | % | |
Moisture Absorption | 24hr | ASTMD570 | 0.090 | % |
平衡,23°C,50%RH | ISO62 | 0.080 | % | |
Melt Mass-Flow Rate | 250°C/2.16kg | ISO1133 | 17 | g/10min |
Melt Volume flow Rate | 250°C/2.16kg | ISO1133 | 13.0 | cm3/10min |
Specific Volume | ASTMD792 | 0.660 | cm³/g |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strain | Yield | ASTMD638 | 2.7 | % |
Break | ASTMD638 | 2.7 | % | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 7580 | Mpa |
Tensile Strength | Yield | ASTMD638 | 120 | Mpa |
Break | ASTMD638 | 120 | Mpa | |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 195 | Mpa |
Break,50.0mmSpan | ASTMD790 | 190 | Mpa | |
Flexural Modulus | ISO178 | 8500 | Mpa | |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17转轮 | ASTMD1044 | 19.0 | mg |
Tensile Stress | 屈服 | ISO527-2/5 | 125 | Mpa |
断裂 | ISO527-2/5 | 125 | Mpa | |
Tensile Strain | 断裂 | ISO527-2/5 | 2.0 | % |
屈服 | ISO527-2/5 | 2.0 | % | |
Tensile Modulus | ISO527-2/1 | 9300 | Mpa | |
Flexural Modulus | ISO178 | 195 | Mpa | |
Tensile Modulus | ASTMD638 | 9300 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 204 | °C |
0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 217 | °C | |
Deflection Temperature Under Load? | 0.45MPa,未退火,6.40mm | ASTMD648 | 216 | °C |
1.8MPa,未退火,3.20mm | ASTMD648 | 203 | °C | |
1.8MPa,未退火,6.40mm | ASTMD648 | 207 | °C | |
0.45MPa,未退火,3.20mm | ASTMD648 | 220 | °C | |
Linear thermal expansion coefficient | TD:-40到40°C | ISO11359-2 | 1.2E-04 | cm/cm/°C |
MD:-40to40°C | ASTME831 | 2.5E-05 | cm/cm/°C | |
MD:60to138°C | ASTME831 | 2.5E-05 | cm/cm/°C | |
MD:-40到40°C | ISO11359-2 | 2.5E-05 | cm/cm/°C | |
TD:-40到40°C | ASTME831 | 1.2E-04 | cm/cm/°C | |
RTIElec | UL746 | 140 | °C | |
Evolution Calendar intelligent importer | UL746 | 140 | °C | |
RTIStr | UL746 | 140 | °C | |
Vicat Softening Temperature | ASTMD152514 | 215 | °C | |
-- | ISO306/B120 | 215 | °C | |
-- | ISO306/A50 | 223 | °C | |
-- | ISO306/B50 | 215 | °C | |
Thermal Conductivity | ISO8302 | 0.19 | W/m/K | |
Ball PressureTest | 125°C | IEC60695-10-2 | Pass |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Comparative Tracking Index | CTI | UL746 | PLC0 | |
Relative Permittivity | 60Hz | IEC60250 | 3.10 | |
50Hz | IEC60250 | 3.10 | ||
1MHz | IEC60250 | 3.10 | ||
Comparative Tracking Index | IEC60112 | 300 | V | |
Dissipation Factor? | 100Hz | ASTMD150 | 2E-03 | |
1MHz | ASTMD150 | 0.020 | ||
50Hz | IEC60250 | 1E-03 | ||
60Hz | IEC60250 | 1E-03 | ||
100Hz | IEC60250 | 1E-03 | ||
1MHz | IEC60250 | 0.010 | ||
Dielectric Strength | 1.00mm15 | IEC60243-1 | 19 | KV/mm |
1.60mm,在油中 | ASTMD149 | 25 | KV/mm | |
0.800mm,在油中 | IEC60243-1 | 28 | KV/mm | |
3.20mm,在油中 | IEC60243-1 | 16 | KV/mm | |
1.60mm,在油中 | IEC60243-1 | 24 | KV/mm | |
3.20mm,inAir | ASTMD149 | 19 | KV/mm | |
Surface Resistivity | IEC60093 | >1.0E+15 | ohms | |
Dielectric Constant | 100Hz | ASTMD150 | 3.80 | |
1MHz | ASTMD150 | 3.70 | ||
Volume Resistivity | IEC60093 | >1.0E+15 | ohms·cm | |
ASTMD257 | >3.2E+16 | ohms·cm | ||
Arc Resistance | ASTMD495 | PLC5 | ||
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC1 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 8.00 | J |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 45 | kJ/m² |
-30°C | ISO179/1eU | 45 | kJ/m² | |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 5.0 | kJ/m² |
-30°C | ISO179/1eA | 5.0 | kJ/m² | |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 45 | kJ/m² |
-30°C | ISO180/1U | 45 | kJ/m² | |
Notched Izod Impact Strength | 23°C | ISO180/1A | 8.0 | kJ/m² |
-30°C | ISO180/1A | 7.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R级 | ASTMD785 | 118 | |
R级 | ISO2039-2 | 118 | ||
Ball Indentation Hardness | H358/30 | ISO2039-1 | 122 | Mpa |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.8mm | UL94 | HB | |
Glow Wire Flammability Index | 1.0mm | IEC60695-2-12 | 750 | °C |
Oxygen Index | ASTMD2863 | 19 | % |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Filler Content | ASTMD229 | 30 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.