Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt Mass-Flow Rate | 300°C/1.2 kg | ASTM D1238 | 7.0 | g/10 min |
Modeling Shrinkage - Flow | | ASTM D955 | 0.50 到 0.70 | % |
Density / Specific Gravity | | ASTM D792 | 1.20 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Flexural Modulus | | ASTM D790 | 2350 | Mpa |
Tensile Elongation | 断裂 | ASTM D638 | > 100 | % |
Flexural Strength | 屈服 | ASTM D790 | 90.2 | Mpa |
Tensile Strength | 屈服 | ASTM D638 | 61.8 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Vicat Softening Temperature | | ASTM D15255 | 153 | °C |
Deflection Temperature Under Load? | 0.45 MPa, 未退火 | ASTM D648 | 144 | °C |
Deflection Temperature Under Load? | 1.8 MPa, 未退火 | ASTM D648 | 133 | °C |
Injection | Test Condition | Test Method | Test Result | Unit |
---|
Drying Time | | | 4.0 | hr |
Rear Temperature | | | 290 到 310 | °C |
Middle Temperature | | | 280 到 300 | °C |
Front Temperature | | | 270 到 290 | °C |
Nozzle Temperature | | | 280 到 300 | °C |
Drying Temperature | | | 120 | °C |
Suggested Max Moisture | | | 0.020 | % |
Processing (Melt) Temp | | | 290 到 310 | °C |
Mold Temperature | | | 60 到 90 | °C |
Hopper Temperature | | | 60 到 80 | °C |
Suggested Max Regrind | | | 20 | % |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | 23°C, 3.18 mm | ASTM D256 | 830 | J/m |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | | ASTM D1003 | 89.0 | % |
Haze | | ASTM D1003 | < 0.80 | % |
Refractive index of light | | ASTM D542 | 1.585 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.