Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50到0.70 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | 屈服 | 内部方法 | 84.3 | Mpa |
Tensile Elongation | 断裂 | 内部方法 | 4.0 | % |
Flexural Modulus | | ASTMD790 | 3730 | Mpa |
Flexural Strength | | ASTMD790 | 128 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,未退火,3.20mm | ASTMD648 | 200 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ASTMD257 | 1E+10 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.