ASA/PC GELOY™ XTPMFR10 WH7E256 SABIC INNOVATIVE US
447
- Properties:Thermal stabilityAntistaticHigh mobility
- Usages:Electrical applicationsAutomotive Applications
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Volume flow Rate | 260°C/2.16kg | ISO1133 | 30.0 | cm3/10min |
Melt Viscosity | 260°C,1500sec^-1 | ISO11443 | 105 | Pa·s |
Density | ISO1183 | 1.18 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Strength | 断裂3 | ASTMD638 | 49.0 | Mpa |
断裂4 | ASTMD638 | 47.0 | Mpa | |
屈服 | ASTMD638 | 60.0 | Mpa | |
屈服 | ASTMD638 | 65.0 | Mpa | |
Tensile Modulus | ASTMD638 | 2680 | Mpa | |
ISO527-2/1 | 2680 | Mpa | ||
Tensile Elongation | 断裂3 | ASTMD638 | 58 | % |
断裂4 | ASTMD638 | 31 | % | |
屈服 | ASTMD638 | 4.0 | % | |
Flexural Modulus | ISO178 | 2730 | Mpa | |
Flexural Strength | ISO178 | 97.0 | Mpa | |
Tensile Stress | 断裂 | ISO527-2/5 | 46.0 | Mpa |
断裂 | ISO527-2/50 | 47.0 | Mpa | |
屈服 | ISO527-2/5 | 61.0 | Mpa | |
屈服 | ISO527-2/50 | 66.0 | Mpa | |
Tensile Strain | 屈服 | ISO527-2/5 | 4.0 | % |
屈服 | ISO527-2/50 | 4.0 | % | |
断裂 | ISO527-2/5 | 50 | % | |
断裂 | ISO527-2/50 | 21 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD:-40到40°C | ISO11359-2 | 6.3E-05 | cm/cm/°C |
TD:-40到40°C | ISO11359-2 | 6.3E-05 | cm/cm/°C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 90.0 | °C |
1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 81.0 | °C | |
Vicat Softening Temperature | -- | ISO306/B50 | 96.0 | °C |
-- | ISO306/B120 | 98.0 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 85.0 | J | |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 13 | kJ/m² |
Notched Izod Impact Strength | -30°C | ASTMD256 | 90 | J/m |
23°C | ASTMD256 | 330 | J/m | |
0°C | ISO180/1A | 12 | kJ/m² | |
23°C | ISO180/1A | 13 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.