Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | | ASTM D-1238 | 11 | g/10min |
Taber wear | H 18轮 | ASTM D-1044 | 168 | mg/1000rev |
Taber wear | CS-17轮 | ASTM D-1044 | 13 | mg/1000rev |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tearing Strength | | ASTM D-1004 | 94 | kN/m |
Tensile Strength | 5%伸长 | ASTM D-638 | 3.8 | Mpa |
Tensile Strength | 10%伸长 | ASTM D-638 | 6.0 | Mpa |
Notched Izod Impact Strength | 23℃ | ASTM D-256 | 不破裂 | J/m |
Tensile Elongation (Break) | | ASTM D-638 | 275 | % |
Tensile Modulus | 23℃ | ASTM D-790 | 117 | Mpa |
Tensile Strength (Break) | | ASTM D-638 | 20.7 | Mpa |
Durometer Hardness | | ASTM D-2240 | 47 | |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melting Temperature | | ASTM D-3418 | 208 | °C |
Vicat Softening Temperature | | ASTM D-1525 | 174 | °C |
Thermal distortion temperature | @0.18Mpa | ASTM D-648 | 45 | °C |
Thermal distortion temperature | @0.5Mpa | ASTM D-648 | 72 | °C |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption (24hr) | | ASTM D-570 | 2.5 | % |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|
Ross Flex | | ASTM D-1052 | >1×10 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.