Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD | 内部方法 | 0.60 | % |
Modeling Shrinkage | TD | 内部方法 | 0.50 | % |
Melt Mass-Flow Rate | 260°C/2.16kg | ASTMD1238 | 36 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | 屈服 | ASTMD638 | 60.0 | Mpa |
Tensile Elongation | 断裂 | ASTMD638 | 3.0 | % |
Flexural Modulus | | ASTMD790 | 3200 | Mpa |
Flexural Strength | | ASTMD790 | 100 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8MPa,未退火 | ASTMD648 | 125 | °C |
Linear thermal expansion coefficient | MD | ASTMD696 | 7E-05 | cm/cm/°C |
Linear thermal expansion coefficient | TD | ASTMD696 | 6E-05 | cm/cm/°C |
Glass Transition Temperature | | 内部方法 | 135 | °C |
Film | Test Condition | Test Method | Test Result | Unit |
---|
Water Vapor Transmission Rate | | ASTMF1249 | 0.090 | g·mm/m²/atm/24hr |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Unnotched Izod Impact Strength | | ASTMD256 | 10.0 | kJ/m² |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | | ASTMD1003 | 90.0 | % |
Haze | | ASTMD1003 | <0.50 | % |
Refractive index of light | | ASTMD542 | 1.540 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.