Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | 210℃/2.16 kg | ISO 1133 | 13 | g/10 min |
Melt index | 190℃/2.16 kg | ISO 1133 | 5.7 | g/10 min |
Ethylene Content | | | 44.0 | wt% |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | | ISO 527-2 | 2300 | Mpa |
Rockwell Hardness | M 计秤 | ISO 2039-2 | 80 | |
Flexural Modulus | | ISO 178 | 4800 | Mpa |
Charpy Notched Impact Strength | | ISO 179 | 2.0 | kJ/m² |
Tensile Stress | 断裂 | ISO 527-2 | 29.0 | Mpa |
Tensile Strain | 断裂 | ISO 527-2 | 11 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Glass Transition Temperature | DSC | DSC | 53.0 | °C |
Peak Crystallization Temperature? | DSC | ISO 3146 | 145 | °C |
Melting temperature (DSC) | | ISO 3146 | 165 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.