AS(SAN) SAN-350 KUMHO KOREA

97

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Density / Specific GravityASTM D-7921.04
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile Strength23℃ASTM D-638780kg/cm2
Tensile Elongation5mm/minASTM D-6384%
Rockwell HardnessASTM D-78586M Scale
Flexural Modulus23℃ASTM D-79035900kg/cm2
Flexural Strength23℃ASTM D-7901050kg/cm2
Izod Impact Strength23℃(73℉)ASTM D-2561.5kg.cm/cm
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Deflection Temperature Under Load?1.86kgf/cm2ASTM D-64893℃(℉)
Vicat Softening Temperature1kgASTM D-1525109°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Arc ResistanceASTM D-149550v/mil
Fire resistance1/16"(1.6mm)UL 94HB
Volume ResistivityASTM D-2571016Ω.cm
ProcessingTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageASTM D-9550.2-0.6%
OtherTest ConditionTest MethodTest ResultUnit
food safetyFDA**符合
PhysicalTest ConditionTest MethodTest ResultUnit
Melt index230℃,3.8kgASTM D-123811g/10min
Melt index200℃,5kgASTM D-12383.5g/10min
Moisture Absorption24hrASTM D-5700.3%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.