Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Density / Specific Gravity | | ISO1183 | 1.48 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 73 | kJ/m² |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 49 | kJ/m² |
Tensile Elongation?(Break) | 23°C | ISO527-2 | 2.5 | % |
Tensile Modulus | 23°C | ISO527-2 | 13400 | Mpa |
Tensile Strength | 23°C | ISO527-2 | 233 | Mpa |
Flexural Modulus | 23°C | ISO178 | 11600 | Mpa |
Flexural Strength | 23°C | ISO178 | 319 | Mpa |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 9.5 | kJ/m² |
Notched Izod Impact Strength | 23°C | ISO180/1A | 8.8 | kJ/m² |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Vicat Softening Temperature | 熔融温度 | ISO11357-3 | 313 | °C |
Deflection Temperature Under Load? | 1.80MPa退火 | ISO75-2/Af | 280 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Insulation strength | 3.20mm | IEC60243-1 | 39 | KV/mm |
Volume Resistivity | | IEC60093 | 1E+15 | Ω.cm |
Flame Rating | Test Condition | Test Method | Test Result | Unit |
---|
Fire rating | | UL-94 | 1.5mm | HB |
Fire rating | | UL-94 | 3.0mm | HB |
Fire rating | | UL-94 | 0.84mm | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.