TPE Hytrel®  5556 DUPONT USA

224
  • Properties:
    Aging resistance
    Weather resistance
    Thermal stability
  • Usages:
    Industrial applications
  • Certificates:
    UL

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Melt indexASTM D-12387.5g/10min
Taber wearH 18轮ASTM D-104464mg/1000rev
Taber wearCS-17轮ASTM D-10446mg/1000rev
Thermal distortion temperature@0.5MpaASTM D-64890°C
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tearing StrengthASTM D-1004158kN/m
Tensile Strength5%伸长ASTM D-6386.9Mpa
Tensile Strength10%伸长ASTM D-63810.3Mpa
Notched Izod Impact Strength23℃ASTM D-256不破裂J/m
Tensile Elongation (Break)ASTM D-638500%
Tensile Modulus23℃ASTM D-790207Mpa
Tensile Strength (Break)ASTM D-63840Mpa
Durometer HardnessASTM D-224055
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Thermal distortion temperature@0.18MpaASTM D-64849°C
Melting TemperatureASTM D-3418203°C
Vicat Softening TemperatureASTM D-1525180°C
PhysicalTest ConditionTest MethodTest ResultUnit
Moisture Absorption (24hr)ASTM D-5700.5%
Other performanceTest ConditionTest MethodTest ResultUnit
Ross FlexASTM D-1052>5×10
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.