Technical Data Sheet
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Elongation?(Break) | -- | ISO-527 | 14.4 | % |
Tensile Strength | -- | ISO-527 | 34 | Mpa |
| -- | ISO-527 | 2700 | Mpa |
Notched Izod Impact Strength | -- | ISO-180 | 2.9 | kj/cm |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Peak Crystallization Temperature? | -- | DSC法 | 161 | °C |
Melting Temperature | -- | DSC法 | 183 | °C |
| -- | H.D.T 法 | 173 | °C |
Glass Transition Temperature | -- | 动粘弹性法 | 69 | °C |
Other | Test Condition | Test Method | Test Result | Unit |
---|
Water Vapor Transmission Rate | 40℃,90%RH | -- | 40~80 | g*30μ/m |
Oxygen Transmission Rate | 20℃,65%RH | -- | 0.4 | CM |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | 230℃*2160g | -- | 1.6 | g/10分 |
Density | -- | -- | 1.19 | g/cm |
Ethylene Content | -- | -- | 32 | 摩尔% |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.