PC/ABS MULTILON® TN-7000F TEIJIN JAPAN
275
- Properties:Flame retardant
- Usages:Computer componentsElectrical applications
- Certificates:UL
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD:4.00mm | 内部方法 | 0.40to0.60 | % |
MD:4.00mm | 内部方法 | 0.40to0.60 | % | |
平行方向 | 0.4-0.6 | % | ||
垂直方向 | 0.4-0.6 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Elongation?(Break) | ISO 527-1,-2 | 20 | % | |
Tensile Stress(Yield) | ISO 527-1,-2 | 63 | Mpa | |
Tensile Stress | 屈服 | ISO527-2/50 | 63.0 | Mpa |
断裂 | ISO527-2/50 | 46.0 | Mpa | |
Tensile Strain | 屈服 | ISO527-2/50 | 2.0 | % |
断裂 | ISO527-2/50 | 20 | % | |
Tensile Modulus | ISO527-2/1 | 3300 | Mpa | |
ISO 527-1,-2 | 3300 | Mpa | ||
Flexural Modulus | ISO 178 | 3200 | Mpa | |
Flexural Strength | ISO 178 | 96 | Mpa | |
Flexural Modulus | ISO178 | 3200 | Mpa | |
Flexural Stress | ISO178 | 96.0 | Mpa | |
Tensile Elongation?(Yield) | ISO 527-1,-2 | 2 | % | |
Izod Impact Strength | 没缺口 | ISO 179 | NB | KJ/m |
带缺口 | ISO 179 | 12 | KJ/m | |
Tensile fracture stress | ISO 527-1,-2 | 46 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Coefficient of Linear Thermal Expansion | 平行方向 | ISO 11359-2 | 0.6 | |
垂直方向 | ISO 11359-2 | 0.7 | ||
Linear thermal expansion coefficient | MD | ISO11359-2 | 6E-05 | cm/cm/°C |
TD | ISO11359-2 | 7E-05 | cm/cm/°C | |
Vicat Softening Temperature | ISO306/B50 | 97.0 | °C | |
Deflection Temperature Under Load? | 0.45MPa,未退火 | ISO75-2/B | 94.0 | °C |
1.8MPa,未退火 | ISO75-2/A | 84.0 | °C | |
-,1.80MPa | ISO 75-1 | 84 | °C | |
-,0.45Mpa | ISO 75-2 | 94 | °C | |
Vicat Softening Temperature | ISO 306 | 97 | °C | |
Flame retardancy | UL94 | V-0 |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC60093 | 1E+16 | ohms |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | ISO179 | NoBreak |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.2mm | UL94 | V-0 | |
1.8mm | UL94 | 5VB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.