Need Help? Contact Us service@plas.com
Get App

AES HW600FR KUMHO KOREA

780

Technical Data Sheet

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMDASTMD9950.30%
Shrinkage rateTDASTMD9950.60%
Melt flow index220℃/10KgASTMD12386.0g/10min
Mechanical performanceTest ConditionTest MethodTest ResultUnit
tensile strength 23°CASTMD63840Mpa
elongation at break 23°CASTMD63815%
bending strength 23°CASTMD79055Mpa
Bending modulus23°CASTMD7902000Mpa
Impact strength of cantilever beam gap23°CASTMD256182J/m
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature1.80MPa未退火ASTMD64880°C
Vicat softening temperatureASTM152586°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.