353
  • Properties:
    transparent
    Crystallization occurs at
    Balanced mold temperature
    No hot spots
  • Usages:
    Higher impact strength
    Can replace transparent A
  • Certificates:
    UL

Technical Data Sheet

physical property Test ConditionTest MethodTest ResultUnit
Mold shrinkage rate3.2mm(0.125in)ASTM D-9550.002-0.006in/in
HazeASTM D-10030.3%
Total transmittanceASTM D-100391%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Flexural yield strengthASTM D-7909700psi
Tensile yield stress/fracture stressASTM D-6386700/7700psi
Yield elongation/fracture elongationASTM D-6385/310%
Flexural modulusASTM D-7902.75×105psi
IZOD notch impact strength23℃/-40℃ASTM D-2567/1.1ft-lb/in
Rockwell hardnessASTM D-785105R
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature1.82MPa(264PSi)ASTM D-64865°C
Hot deformation temperature0.45MPa(66PSi)ASTM D-64873°C
Vicat softening temperature1kg负荷ASTM D-152585°C
Combustibility3.0mmUL 94V-2
Other performanceTest ConditionTest MethodTest ResultUnit
Intrinsic viscosity0.72
Basic performanceTest ConditionTest MethodTest ResultUnit
Melt index230℃,5kg15g/10min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.