TPE Hytrel® 8238 DuPont, European Union
409
- Properties:High temperature resistan
- Usages:Engine partsCable sheathWire and cableJointHose
- Certificates:UL
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | TD | ISO294-4 | 1.6 | % |
MD | ISO294-4 | 1.6 | % | |
Water absorption rate | 23°C,24hr | ISO62 | 0.30 | % |
饱和,23°C,2.00mm | ISO62 | 0.60 | % | |
平衡,23°C,2.00mm,50%RH | ISO62 | 0.20 | % | |
MediumDensity | 1.13 | g/cm³ | ||
SpecificHeatCapacity of Melt | 2150 | J/kg/°C | ||
ThermalConductivityofMelt | 0.15 | W/m/K | ||
Melt mass flow rate | 240°C/2.16kg | ISO1133 | 13 | g/10min |
Melt volume flow rate | 240°C/2.16kg | ISO1133 | 11.5 | cm3/10min |
Density/specific gravity | ISO1183 | 1.28 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Nominal tensile fracture strain | ISO527-2 | 340 | % | |
Tensile stress | 屈服 | ISO527-2 | 38.0 | Mpa |
断裂 | ISO527-2 | 46.0 | Mpa | |
10%应变 | ISO527-2 | 34.0 | Mpa | |
50%应变 | ISO527-2 | 28.0 | Mpa | |
100%应变 | ISO527-2 | 26.0 | Mpa | |
Tensile strain | 屈服 | ISO527-2 | 19 | % |
断裂 | ISO527-2 | >300 | % | |
Tensile modulus | ISO527-2 | 1200 | Mpa | |
Bending modulus | ISO178 | 1150 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,未退火 | ISO75-2/B | 105 | °C |
1.8MPa,未退火 | ISO75-2/A | 45.0 | °C | |
Brittle temperature | ISO974 | -84.0 | °C | |
Vicat softening temperature | -- | ISO306/A50 | 213 | °C |
-- | ISO306/B50 | 150 | °C | |
Linear coefficient of thermal expansion | TD:-40to23°C | ISO11359-2 | 1E-04 | cm/cm/°C |
TD:EffectiveThermalDiffusivity | ISO11359-2 | 5.44E-08 | m²/s | |
MD:-- | ISO11359-2 | 1.5E-04 | cm/cm/°C | |
MD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C | |
TD:-- | ISO11359-2 | 1.4E-04 | cm/cm/°C | |
Glass transition temperature 2 | ISO11357-2 | 50.0 | °C | |
Melting temperature 2 | ISO11357-3 | 221 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric strength | IEC60243-1 | 21 | KV/mm | |
Relative permittivity | 100Hz | IEC60250 | 4.00 | |
1MHz | IEC60250 | 3.70 | ||
Leakage Trace Index | IEC60112 | 600 | V | |
Surface resistivity | IEC60093 | >1.0E+15 | ohms | |
Volume resistivity | IEC60093 | >1.0E+15 | ohms·cm | |
Dissipation factor | 100Hz | IEC60250 | 0.010 | |
1MHz | IEC60250 | 0.018 |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
tear strength | 横向流量 | ISO34-1 | 210 | kN/m |
流量 | ISO34-1 | 230 | kN/m |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -40°C | ISO179/1eA | 5.0 | kJ/m² |
-30°C | ISO179/1eA | 5.0 | kJ/m² | |
23°C | ISO179/1eA | 15 | kJ/m² | |
Impact strength of cantilever beam gap | -40°C | ISO180/1A | 5.5 | kJ/m² |
23°C | ISO180/1A | 11 | kJ/m² | |
Tensile impact strength | 23°C | ISO8256/1 | 57.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | 邵氏D | ISO868 | 76 | |
邵氏D,15秒 | ISO868 | 70 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.9mm | UL94 | HB | |
1.5mm | UL94 | HB | ||
0.9mm | IEC60695-11-10,-20 | HB | ||
1.5mm | IEC60695-11-10,-20 | HB | ||
Extreme Oxygen Index | ISO4589-2 | 22 | % | |
FMVSS flammability | FMVSS302 | SE |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
EmissionofOrganicCompounds | VDA277 | 550 | µgC/g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.