Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Melt flow rate | 250°C/5.0 kg | ASTM D1238 | 11 | g/10 min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Bending modulus 6 | 100 mm 跨距 | ASTM D790 | 80.0 | Mpa |
Bending modulus 6 | -- | ISO 178 | 90.0 | Mpa |
elongation | 断裂 1 | UL 1581 | 210 | % |
elongation | 断裂 4 | ASTM D638 | 120 | % |
elongation | 断裂, 113°C 5 | UL 1581 | 150 | % |
elongation | 断裂 | ISO 527-2/50 | 120 | % |
Tensile strength | 断裂 1 | UL 1581 | 16.0 | Mpa |
Tensile strength | 断裂 2 | ASTM D638 | 12.0 | Mpa |
Tensile strength | 断裂, 113°C 3 | UL 1581 | 17.0 | Mpa |
Tensile strength | 断裂 | ISO 527-2/50 | 13.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Brittle temperature | | ASTM D746 | < -40.0 | °C |
UL temperature rating 7 | | UL 1581 | 80 | °C |
Heat Deformation | 100°C | UL 1581 | 16 | % |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | | IEC 60093 | 3.8E+15 | ohms·cm |
Dissipation factor | 50 Hz | IEC 60250 | 0.030 | |
Dissipation factor | 60 Hz | IEC 60250 | 0.030 | |
Dissipation factor | 1 MHz | IEC 60250 | 4.0E-3 | |
Dielectric strength | 2.00 mm, 在油中 | IEC 60243-1 | 23 | KV/mm |
Relative permittivity | 50 Hz | IEC 60250 | 2.80 | |
Relative permittivity | 60 Hz | IEC 60250 | 2.80 | |
Relative permittivity | 1 MHz | IEC 60250 | 2.80 | |
Leakage Trace Index | | IEC 60112 | 600 | V |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore hardness | 邵氏 A, 30 秒 | ASTM D2240 | 80 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
Burning wire flammability index | 3.0 mm | IEC 60695-2-12 | 650 | °C |
Extreme Oxygen Index | | ISO 4589-2 | 26 | % |
Extreme Oxygen Index | VW-1 1 | UL 1581 | Pass | |
Hot filament ignition temperature | 3.0 mm | IEC 60695-2-13 | 750 | °C |
UL flame retardant rating | 4.0 mm | UL 94 | V-0 | |
Smoke density 9 | Flaming, Ds max : 500.0 µm | ASTM E662 | 140 | |
Smoke density 9 | Non-Flaming, Ds max : 500.0 µm | ASTM E662 | 95 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.