PCTG Tritan™ EX401 EASTMAN USA
290
- Properties:Chemical resistanceHydrolysis resistance
- Usages:Electrical applicationsHousehold daily necessiti
- Certificates:MSDS
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:BlowMolded | 内部方法 | 1.2to1.6 | % |
MD:注塑 | ASTMD955 | 0.50to0.70 | % | |
Density/specific gravity | ASTMD792 | 1.17 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | 23°C | ASTMD638 | 1590 | Mpa |
23°C | ISO527-2 | 1620 | Mpa | |
elongation | 屈服,23°C2 | 内部方法 | 7.0 | % |
屈服,23°C3 | 内部方法 | 6.5 | % | |
屈服,23°C | ASTMD638 | 7.0 | % | |
断裂,23°C | ASTMD638 | 140 | % | |
Bending modulus | 23°C | ASTMD790 | 1590 | Mpa |
23°C | ISO178 | 1530 | Mpa | |
bending strength | 屈服,23°C | ASTMD790 | 66.0 | Mpa |
Tensile stress | 断裂,23°C | ISO527-2 | 49.0 | Mpa |
屈服,23°C2 | 内部方法 | 44.0 | Mpa | |
屈服,23°C3 | 内部方法 | 45.0 | Mpa | |
屈服,23°C | ISO527-2 | 45.0 | Mpa | |
Tensile strain | 断裂,23°C | ISO527-2 | 130 | % |
屈服,23°C | ISO527-2 | 7.0 | % | |
Tensile strength | 屈服,23°C | ASTMD638 | 44.0 | Mpa |
断裂,23°C | ASTMD638 | 53.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,未退火 | ASTMD648 | 109 | °C |
1.8MPa,未退火 | ASTMD648 | 92.0 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of cantilever beam gap | -40°C | ASTMD256 | 130 | J/m |
23°C | ASTMD256 | 650 | J/m | |
23°C3 | 内部方法 | 640 | J/m | |
23°C2 | 内部方法 | 650 | J/m | |
-40°C | ISO180 | 14 | kJ/m² | |
23°C | ISO180 | 66 | kJ/m² | |
-40°C | ASTMD4812 | NoBreak | ||
23°C | ASTMD4812 | NoBreak | ||
Dart impact equipped with measuring instruments | -40°C,EnergyatMaxLoad | ASTMD3763 | 63.0 | J |
23°C,EnergyatMaxLoad | ASTMD3763 | 59.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R计秤,23°C | ASTMD785 | 115 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Haze | --2 | 内部方法 | <1.0 | % |
-- | ASTMD1003 | <1.0 | % | |
transmissivity | 总计 | ASTMD1003 | 92.0 | % |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FillVolumeShrinkage4 | Boiling,1hr | 内部方法 | <1.0 | % |
Boiling,2hr | 内部方法 | <1.5 | % | |
Dishwasher | 内部方法 | <1.0 | % | |
MicrowaveBoiling-OvenPower4 | 内部方法 | <2200 | Watts | |
ThermalShock-WaterImmersion4 | 35to98°C | 内部方法 | Noeffect | |
MicrowaveSteamSterilization-TotalEnergy4 | 内部方法 | <11200 | W-min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.