physical property | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | 190℃/2.16 kg | ASTM D1238 | 0.75 | g/10 min |
Resistance to environmental stress cracking | 100℃, 100% Igepal, F0 | ASTM D1693 | > 48.0 | hr |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile strength | | ASTM D638 | 23.4 | Mpa |
elongation | 断裂 | ASTM D638 | 500 | % |
Tensile strength retention rate -48 hours | 100℃ | STM D638 | 90 | % |
Elongation retention rate -48 hours | 100℃ | STM D638 | 90 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Brittle temperature | | ASTM D746 | -76.0 | °C |
Heat-resistant stress crack | F0 | ASTM D2951 | > 96 | hr |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | 23℃ | ASTM D257 | > 1.0E+15 | ohm·cm |
Dielectric constant | 1 MHz | ASTM D257 | 2.32 | |
Dissipation factor | 1 MHz | ASTM D1531 | 0.000060 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.