Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Shrinkage rate | MD:3.20mm | 内部方法 | 0.50到0.70 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile strength | 屈服 | 内部方法 | 84.3 | Mpa |
elongation | 断裂 | 内部方法 | 4.0 | % |
Bending modulus | | ASTMD790 | 3730 | Mpa |
bending strength | | ASTMD790 | 128 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 0.45MPa,未退火,3.20mm | ASTMD648 | 200 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface resistivity | | ASTMD257 | 1E+10 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.