Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Mold shrinkage rate | 3.2mm | ASTM D-955 | 2-5 | |
Loss factor | 60Hz | ASTM D-150 | 0.0016 | |
enhance | | | 20 | % |
Density/specific gravity | | ASTM D-792 | 1.23 | |
Flame retardancy | | UL 94 | V-1 | |
Flame retardancy | | UL 94 | 1.5 | mm |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
tensile strength | 屈服点,3.2mm | ASTM D-638 | 107 | Mpa |
tensile strength | 断裂点,3.2mm | ASTM D-638 | 5 | Mpa |
Rockwell hardness | | ASTM D-785 | 106 | |
Bending modulus | 6.4mm | ASTM D-790 | 5719 | Mpa |
bending strength | 6.4mm | ASTM D-790 | 152 | Mpa |
Gap impact strength | 23°C | ASTM D-256 | 107 | J/m |
Gap impact strength | -40°C | ASTM D-256 | 96 | J/m |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 1.8MPa | ASTM D-648 | 132 | °C |
Hot deformation temperature | 0.45MPa | ASTM D-648 | 137 | °C |
Coefficient of linear expansion | | ASTM E-831 | 3.6×10 | 1/°C |
UL long-term use temperature | 电气 | UL 746B | 110 | °C |
UL long-term use temperature | 含冲击 | UL 746B | 105 | °C |
UL long-term use temperature | 无冲击 | UL 746B | 110 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric constant | 60Hz | ASTM D-150 | 2.98 | |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|
Water absorption rate | 24hrs | ASTM D-570 | 0.06 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.