PETG Eastar™ DS2010 EASTMAN USA
377
- Properties:High transparencyHigh toughness
- Usages:chipsporting goods
- Certificates:UL
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | ASTMD955 | 0.20to0.60 | % |
Density/specific gravity | 23°C | ISO1183 | 1.19 | g/cm³ |
ASTMD792 | 1.20 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress | 断裂,23°C | ISO527-2 | 49.0 | Mpa |
屈服,23°C | ISO527-2 | 47.0 | Mpa | |
Tensile strain | 断裂,23°C | ISO527-2 | 210 | % |
屈服,23°C | ISO527-2 | 4.0 | % | |
Tensile strength | 屈服,23°C | ASTMD638 | 46.0 | Mpa |
断裂,23°C | ASTMD638 | 53.0 | Mpa | |
Bending stress | 23°C | ISO178 | 64.0 | Mpa |
elongation | 断裂,23°C | ASTMD638 | 310 | % |
屈服,23°C | ASTMD638 | 5.0 | % | |
Bending modulus | 23°C | ASTMD790 | 1900 | Mpa |
23°C | ISO178 | 1750 | Mpa | |
bending strength | 屈服,23°C | ASTMD790 | 67.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,未退火 | ASTMD648 | 73.0 | °C |
0.45MPa,未退火 | ISO75-2/B | 73.0 | °C | |
1.8MPa,未退火 | ASTMD648 | 65.0 | °C | |
1.8MPa,未退火 | ISO75-2/A | 66.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | ASTMD257 | 1E+17 | ohms | |
Dielectric constant | 23°C,1kHz | ASTMD150 | 2.60 | |
23°C,10kHz | ASTMD150 | 2.60 | ||
23°C,100kHz | ASTMD150 | 2.50 | ||
23°C,1MHz | ASTMD150 | 2.50 | ||
Arc resistance | ASTMD495 | 123 | sec | |
Volume resistivity | 23°C | ASTMD257 | 1E+17 | ohms·cm |
Dielectric strength 2 | 23°C | ASTMD149 | 17 | KV/mm |
Dissipation factor | 23°C,1kHz | ASTMD150 | 6E-03 | |
23°C,10kHz | ASTMD150 | 0.012 | ||
23°C,100kHz | ASTMD150 | 0.015 | ||
23°C,1MHz | ASTMD150 | 0.015 | ||
Leakage Trace Index | ASTMD3638 | 700 | V |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of cantilever beam gap | -40°C | ASTMD256 | 60 | J/m |
23°C | ASTMD256 | 370 | J/m | |
-40°C | ISO180 | 6.3 | kJ/m² | |
23°C | ISO180 | 30 | kJ/m² | |
-40°C | ASTMD4812 | NoBreak | ||
23°C | ASTMD4812 | NoBreak | ||
Multi axis Instrumented Impact Energy | -40°C,能量到力量峰值 | ISO6603-2 | 55.0 | J |
23°C,能量到力量峰值 | ISO6603-2 | 71.0 | J | |
Dart impact equipped with measuring instruments | -40°C,EnergyatPeakLoad | ASTMD3763 | 48.0 | J |
23°C,EnergyatPeakLoad | ASTMD3763 | 45.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R计秤,23°C | ASTMD785 | 105 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
transmissivity | 总计 | ASTMD1003 | 91.0 | % |
Regular | ASTMD1003 | 89.0 | % | |
Haze | ASTMD1003 | 0.30 | % |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FlameRating | 3.0mm,AT | UL94 | V-2 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.