Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Shrinkage rate | 流量 | ISO 294-4 | 0.5-0.7 | % |
Dissolved volume flow rate | 230℃/2.16kg | ISO 1133 | 9.00 | cm3/10min |
Rockwell hardness | | ISO 2039-2 | 106 | Mpa |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile modulus | 23 ℃ | ISO 527-2 | 2100 | Mpa |
Yield tensile stress | 23 ℃ | ISO 527-2 | 51 | Mpa |
Bending modulus | 23 ℃ | ISO 178 | 2450 | Mpa |
bending strength | 23 ℃ | ISO 178 | 86 | Mpa |
Charpy Notched Impact Strength | 23 ℃ | ISO 179 | 50 | kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 1.8MPa | ISO 75-2/A | 94 | °C |
Linear expansion coefficient | | ISO 11359-2 | 0.000095 | cm/cm/℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.