Technical Data Sheet
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Notched Impact Strength | -30℃ | KJ/m | ISO 179/1eA | 2.40 |
Charpy Notched Impact Strength | 23℃ | KJ/m | ISO 179/1eA | 26.6 |
Charpy impact strength | -30℃ | KJ/m | ISO 179/1eU | 35.5 |
Charpy impact strength | 23℃ | KJ/m | ISO 179/1eU | No Break |
Tensile yield stress | | MPa | ISO 527-2 | |
Tensile yield strain | | % | ISO 527-2 | 6.0 |
Tensile modulus | | MPa | ISO 527-2 | 2300 |
Tensile fracture strain | | % | ISO 527-2 | 18 |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Glass transition temperature | | ℃ | ISO 11357-2 | |
burning | 3.20mm | | ISO 1210 | HB |
Linear coefficient of thermal expansion | Flow | cm/cm/℃ | ISO 11359-2 | 0.000071 |
Linear coefficient of thermal expansion | Transverse | cm/cm/℃ | ISO 11359-2 | 0.000071 |
Vicat softening temperature | 50℃/h,B(50N) | ℃ | ISO 306 | 95.4 |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Relative permittivity | 1MHz | | IEC 60250 | 3.20 |
Dielectric loss factor | 1MHz | | IEC 60250 | 0.028 |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|
Density/specific gravity | | Kg/m | ISO 1183 | |
Melt index | 220℃/10.0kg | cm | ISO 1133 | 4.60 |
Water absorption rate | Soultion | % | ISO 62 | 0.31 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.