Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP JR-3070HP PRIME POLYMER JAPAN
PRIME POLYPRO
Household goods、Food containers
soft、High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
physical property
Test Condition
Test Method
Unit
PP/PRIME POLYMER JAPAN/JR-3070HP
Melt mass flow rate
230°C/2.16kg
ISO1133
g/10min
3
Mechanical performance
Test Condition
Test Method
Unit
PP/PRIME POLYMER JAPAN/JR-3070HP
impact strength
23℃
ISO 179
kJ/m²
7
impact strength
-20℃
ISO 179
kJ/m²
2
Tensile modulus
ISO527-2
Mpa
7
tensile strength
ISO 527
Mpa
2
Tensile strain
断裂
ISO527-2
%
4
Tensile stress
屈服
ISO527-2
Mpa
2
Rockwell hardness
ISO 2039-2
R scale
4
elongation
断裂
ISO 527
%
4
Bending modulus
ISO 527
Mpa
7
Thermal performance
Test Condition
Test Method
Unit
PP/PRIME POLYMER JAPAN/JR-3070HP
Hot deformation temperature
0.45MPa
ISO 75
°C
6
Hot deformation temperature
0.45MPa,未退火
ISO75-2/B
°C
6
Impact performance
Test Condition
Test Method
Unit
PP/PRIME POLYMER JAPAN/JR-3070HP
Impact strength of simply supported beam without notch
-20°C
ISO179
kJ/m²
2
Impact strength of simply supported beam without notch
23°C
ISO179
kJ/m²
7
Basic performance
Test Condition
Test Method
Unit
PP/PRIME POLYMER JAPAN/JR-3070HP
density
ISO 1183
g/cm³
0
Melt index
230℃
ISO 1133
g/10min
3