Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPV 8211-55B100 CELANESE USA
Santoprene™
Kitchen utensils、Electrical appliances、Engine hood parts、Movable hinge、Home appliance components、Household appliances、Mirror frame、Seals、Fatigue relief supplies、Automotive sector、Soft handle、sporting goods、Consumer goods sector、Bonding、Adhesive resin、Smart phone
wear resistant、Aging resistance、UV resistance、Weather resistance、High mobility、Recyclable materials、Good adhesion、Excellent surface finish、Good forming performance、Good flexibility、Good colorability、Ozone resistance、Good appearance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
ageing
Test Condition
Test Method
Unit
TPV/CELANESE USA/8211-55B100
Changes in tensile stress during fracture
23°C,168hr,inEthanol,95%
ISO1817
%
-
Changes in tensile stress during fracture
23°C,168hr,inHydrochloricAcid,10%
ISO1817
%
-
Changes in tensile stress during fracture
23°C,168hr,inIRM903Oil
ISO1817
%
-
Changes in tensile stress during fracture
23°C,168hr,inSodiumHydroxide,50%
ISO1817
%
-
Changes in tensile stress during fracture
23°C,168hr,在水中
ISO1817
%
-
Change rate of ultimate elongation
23°C,168hr,inEthanol,95%
ASTMD471
%
-
Change rate of ultimate elongation
23°C,168hr,inHydrochloricAcid,10%
ASTMD471
%
-
Change rate of ultimate elongation
23°C,168hr,inIRM903Oil
ASTMD471
%
-
Change rate of ultimate elongation
23°C,168hr,inSodiumHydroxide,50%
ASTMD471
%
-
Change rate of ultimate elongation
23°C,168hr,在水中
ASTMD471
%
-
Change rate of ultimate elongation in air
100°C,168hr
ASTMD573
%
-
Change rate of ultimate elongation in air
125°C,168hr
ASTMD573
%
-
Change rate of tensile strength in air
100°C,168hr
ASTMD573
%
-
Change rate of tensile strength in air
125°C,168hr
ASTMD573
%
-
Change rate of tensile strength in air
100°C,168hr
ISO188
%
-
Change rate of tensile strength in air
125°C,168hr
ISO188
%
-
Change rate of tensile strength
23°C,168hr,inEthanol,95%
ASTMD471
%
-
Change rate of tensile strength
23°C,168hr,inHydrochloricAcid,10%
ASTMD471
%
-
Change rate of tensile strength
23°C,168hr,inIRM903Oil
ASTMD471
%
-
Change rate of tensile strength
23°C,168hr,inSodiumHydroxide,50%
ASTMD471
%
1
Change rate of tensile strength
23°C,168hr,在水中
ASTMD471
%
2
Change rate of tensile strength
23°C,168hr,inEthanol,95%
ISO1817
%
-
Change rate of tensile strength
23°C,168hr,inHydrochloricAcid,10%
ISO1817
%
-
Change rate of tensile strength
23°C,168hr,inIRM903Oil
ISO1817
%
-
Change rate of tensile strength
23°C,168hr,inSodiumHydroxide,50%
ISO1817
%
1
Change rate of tensile strength
23°C,168hr,在水中
ISO1817
%
2
Changes in tensile stress during fracture in air
100°C,168hr
ISO188
%
-
Changes in tensile stress during fracture in air
125°C,168hr
ISO188
%
-
elastomer
Test Condition
Test Method
Unit
TPV/CELANESE USA/8211-55B100
CompressionSet2
125°C,70hr
ASTMD395B
%
5
CompressionSet3
125°C,70hr
ISO815
%
5
Elongation rate - lateral flow rate
断裂,23°C
ASTMD412
%
6
Elongation rate - lateral flow rate
断裂,23°C
ISO37
%
6