Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU 2355-95A LUBRIZOL USA
Pearlthane®
film、Laminate、Cable、Coating application
Flame retardant、Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
physical property
Test Condition
Test Method
Unit
TPU/LUBRIZOL USA/2355-95A
Melt mass flow rate
190°C/8.7kg
ASTMD1238
g/10min
1
Shrinkage rate
MD
ASTMD955
%
0
Shrinkage rate
TD
ASTMD955
%
0
Mechanical performance
Test Condition
Test Method
Unit
TPU/LUBRIZOL USA/2355-95A
Taber abraser
1000g,H-22转轮
ASTMD1044
mg
4
Bending modulus
3.20mm
ASTMD790
Mpa
8
Thermal performance
Test Condition
Test Method
Unit
TPU/LUBRIZOL USA/2355-95A
Glass transition temperature
DSC
°C
-
Vicat softening temperature
ASTMD15252
°C
8
Linear coefficient of thermal expansion
MD
ASTMD696
cm/cm/°C
1
elastomer
Test Condition
Test Method
Unit
TPU/LUBRIZOL USA/2355-95A
Tensile strength
断裂,3.20mm
ASTMD412
Mpa
3
Tensile stress
50%应变,3.20mm
ASTMD412
Mpa
8
Tensile stress
100%应变,3.20mm
ASTMD412
Mpa
9
Tensile stress
300%应变,3.20mm
ASTMD412
Mpa
2
elongation
断裂,3.20mm
ASTMD412
%
4
Tear strength 1
3.20mm
ASTMD624
kN/m
1
Permanent compression deformation
25°C,22hr
ASTMD395B
%
3
Permanent compression deformation
70°C,22hr
ASTMD395B
%
8