Need Help? Contact Us service@plas.com
Get App

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP H030 GP SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

physical property
Test Condition
Test Method
Unit
PP/SIBUR RUSSIA/H030 GP
Melt index
230℃/2.16 kg
Internal Method
g/10 min
3
Mechanical performance
Test Condition
Test Method
Unit
PP/SIBUR RUSSIA/H030 GP
Tensile strain
屈服
Internal Method
%
1
Tensile stress
屈服
Internal Method
Mpa
3
Bending modulus
Internal Method
Mpa
1
Impact strength of cantilever beam gap
23℃
Internal Method
kJ/m²
2
Thermal performance
Test Condition
Test Method
Unit
PP/SIBUR RUSSIA/H030 GP
Hot deformation temperature
0.45 MPa, 未退火
Internal Method
°C
8
Vicat softening temperature
Internal Method
°C
1