Need Help? Contact Us service@plas.com
Get App

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TPU 985 COVESTRO GERMANY
Desmopan® 
Engineering accessories
wear resistant、High transparency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

physical property
Test Condition
Test Method
Unit
TPU/COVESTRO GERMANY/985
Shrinkage rate
MD:2.54mm
ASTMD955
%
0
Shrinkage rate
TD:2.54mm
ASTMD955
%
0
Shrinkage rate
TD:2.54mm
ISO2577
%
0
Shrinkage rate
MD:2.54mm
ISO2577
%
0
Mechanical performance
Test Condition
Test Method
Unit
TPU/COVESTRO GERMANY/985
Taber abraser
1000Cycles,1000g,H-18转轮
ISO4649
mg
3
Taber abraser
1000Cycles,1000g,H-18转轮
ASTMD1044
mg
3
Bending modulus
-30°C
ASTMD790
Mpa
5
Bending modulus
23°C
ASTMD790
Mpa
2
Bending modulus
-30°C
ISO178
Mpa
5
Bending modulus
23°C
ISO178
Mpa
2
Thermal performance
Test Condition
Test Method
Unit
TPU/COVESTRO GERMANY/985
Glass transition temperature
DMA
°C
-
Brittle temperature
ASTMD746
°C
<
Brittle temperature
ISO974
°C
<
Vicat softening temperature
ASTMD15254
°C
8
Vicat softening temperature
ISO306/50
°C
8
ageing
Test Condition
Test Method
Unit
TPU/COVESTRO GERMANY/985
Changes in tensile stress during fracture
23°C,70hr,inReferenceFuelA(Isooctane)
BTM 00117
%
-
Changes in tensile stress during fracture
23°C,70hr,甲醇
BTM 00117
%
-
Changes in tensile stress during fracture
23°C,168hr,inReferenceFuelA(Isooctane)
BTM 00117
%
0
Changes in tensile stress during fracture
23°C,168hr,甲醇
BTM 00117
%
-
Changes in tensile stress during fracture
23°C,336hr,inReferenceFuelA(Isooctane)
BTM 00117
%
3
Changes in tensile stress during fracture
23°C,336hr,inReferenceFuelC
BTM 00117
%
-
Changes in tensile stress during fracture
23°C,504hr,inReferenceFuelA(Isooctane)
BTM 00117
%
8
Changes in tensile stress during fracture
23°C,504hr,inReferenceFuelC
BTM 00117
%
-
Changes in tensile stress during fracture
100°C,70hr,在ASTM#1油中
BTM 00117
%
1
Changes in tensile stress during fracture
100°C,70hr,在ASTM#3油中
BTM 00117
%
1
Changes in tensile stress during fracture
100°C,168hr,inASTM#1Oil
BTM 00117
%
7
Changes in tensile stress during fracture
100°C,168hr,inASTM#3Oil
BTM 00117
%
1
Changes in tensile stress during fracture
100°C,336hr,inASTM#1Oil
BTM 00117
%
1
Changes in tensile stress during fracture
100°C,336hr,inASTM#3Oil
BTM 00117
%
2
Changes in tensile stress during fracture
100°C,504hr,inASTM#1Oil
BTM 00117
%
1
Changes in tensile stress during fracture
100°C,504hr,inASTM#3Oil
BTM 00117
%
2
Change rate of ultimate elongation
100°C,504hr,inASTM#3Oil
ASTMD471
%
2
Change rate of ultimate elongation
23°C,336hr,inReferenceFuelC
ASTMD471
%
-
Change rate of ultimate elongation
23°C,504hr,inReferenceFuelA(Isooctane)
ASTMD471
%
8
Change rate of ultimate elongation
23°C,504hr,inReferenceFuelC
ASTMD471
%
-
Change rate of ultimate elongation
100°C,70hr,在ASTM#1油中
ASTMD471
%
1
Change rate of ultimate elongation
100°C,70hr,在ASTM#3油中
ASTMD471
%
1
Change rate of ultimate elongation
100°C,168hr,inASTM#1Oil
ASTMD471
%
7
Change rate of ultimate elongation
100°C,168hr,inASTM#3Oil
ASTMD471
%
1
Change rate of ultimate elongation
100°C,336hr,inASTM#1Oil
ASTMD471
%
1
Change rate of ultimate elongation
100°C,336hr,inASTM#3Oil
ASTMD471
%
2
Change rate of ultimate elongation
100°C,504hr,inASTM#1Oil
ASTMD471
%
1
Change rate of ultimate elongation
23°C,70hr,inReferenceFuelA(Isooctane)
ASTMD471
%
-
Change rate of ultimate elongation
23°C,70hr,甲醇
ASTMD471
%
-
Change rate of ultimate elongation
23°C,168hr,inReferenceFuelA(Isooctane)
ASTMD471
%
0
Change rate of ultimate elongation
23°C,168hr,甲醇
ASTMD471
%
-
Change rate of ultimate elongation
23°C,336hr,inReferenceFuelA(Isooctane)
ASTMD471
%
3
Change rate of ultimate elongation in air
100°C,168hr
ASTMD573
%
1
Change rate of ultimate elongation in air
100°C,336hr
ASTMD573
%
2
Change rate of ultimate elongation in air
100°C,504hr
ASTMD573
%
1
Change rate of ultimate elongation in air
125°C,70hr
ASTMD573
%
1
Change rate of ultimate elongation in air
125°C,168hr
ASTMD573
%
1
Change rate of ultimate elongation in air
125°C,336hr
ASTMD573
%
1
Change rate of ultimate elongation in air
125°C,504hr
ASTMD573
%
2
Change rate of ultimate elongation in air
100°C,70hr
ASTMD573
%
1
Change rate of tensile strength in air
100°C,70hr
ASTMD573
%
4
Change rate of tensile strength in air
100%Strain,100°C,70hr
ASTMD573
%
-
Change rate of tensile strength in air
300%Strain,100°C,70hr
ASTMD573
%
0
Change rate of tensile strength in air
100°C,168hr
ASTMD573
%
7
Change rate of tensile strength in air
100%Strain,100°C,168hr
ASTMD573
%
-
Change rate of tensile strength in air
300%Strain,100°C,168hr
ASTMD573
%
7
Change rate of tensile strength in air
100°C,336hr
ASTMD573
%
3
Change rate of tensile strength in air
100%Strain,100°C,336hr
ASTMD573
%
2
Change rate of tensile strength in air
300%Strain,100°C,336hr
ASTMD573
%
8
Change rate of tensile strength in air
125°C,168hr
ISO216
%
-
Change rate of tensile strength in air
100%应变125°C,168hr
ISO216
%
4
Change rate of tensile strength in air
300%Strain125°C,168hr
ISO216
%
8
Change rate of tensile strength in air
125°C,336hr
ISO216
%
-
Change rate of tensile strength in air
100%Strain125°C,336hr
ISO216
%
-
Change rate of tensile strength in air
300%Strain125°C,336hr
ISO216
%
-
Change rate of tensile strength in air
125°C,504hr
ISO216
%
-
Change rate of tensile strength in air
100%Strain125°C,504hr
ISO216
%
-
Change rate of tensile strength in air
300%Strain125°C,504hr
ISO216
%
-
Change rate of tensile strength in air
100%Strain,125°C,336hr
ASTMD573
%
-
Change rate of tensile strength in air
300%Strain,125°C,336hr
ASTMD573
%
-
Change rate of tensile strength in air
125°C,504hr
ASTMD573
%
-
Change rate of tensile strength in air
100%Strain,125°C,504hr
ASTMD573
%
-
Change rate of tensile strength in air
300%Strain,125°C,504hr
ASTMD573
%
-
Change rate of tensile strength in air
100°C,70hr
ISO216
%
4
Change rate of tensile strength in air
100%Strain100°C,70hr
ISO216
%
-
Change rate of tensile strength in air
300%Strain100°C,70hr
ISO216
%
0
Change rate of tensile strength in air
100°C,168hr
ISO216
%
7
Change rate of tensile strength in air
100%Strain100°C,168hr
ISO216
%
-
Change rate of tensile strength in air
100°C,504hr
ASTMD573
%
-
Change rate of tensile strength in air
100%Strain,100°C,504hr
ASTMD573
%
-
Change rate of tensile strength in air
300%Strain,100°C,504hr
ASTMD573
%
1
Change rate of tensile strength in air
125°C,70hr
ASTMD573
%
-
Change rate of tensile strength in air
100%Strain,125°C,70hr
ASTMD573
%
4
Change rate of tensile strength in air
300%Strain,125°C,70hr
ASTMD573
%
2
Change rate of tensile strength in air
125°C,168hr
ASTMD573
%
-
Change rate of tensile strength in air
100%Strain,125°C,168hr
ASTMD573
%
4
Change rate of tensile strength in air
300%Strain,125°C,168hr
ASTMD573
%
8
Change rate of tensile strength in air
125°C,336hr
ASTMD573
%
-
Change rate of tensile strength in air
300%Strain100°C,168hr
ISO216
%
7
Change rate of tensile strength in air
100°C,336hr
ISO216
%
3
Change rate of tensile strength in air
100%Strain100°C,336hr
ISO216
%
2
Change rate of tensile strength in air
300%Strain100°C,336hr
ISO216
%
8
Change rate of tensile strength in air
100°C,504hr
ISO216
%
-
Change rate of tensile strength in air
100%Strain100°C,504hr
ISO216
%
-
Change rate of tensile strength in air
300%Strain100°C,504hr
ISO216
%
1
Change rate of tensile strength in air
125°C,70hr
ISO216
%
-
Change rate of tensile strength in air
100%Strain125°C,70hr
ISO216
%
4
Change rate of tensile strength in air
300%Strain125°C,70hr
ISO216
%
2
Change rate of tensile strength
300%Strain,23°C,504hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
100°C,70hr,在ASTM#1油中
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,70hr,inASTM#1Oil
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,70hr,inASTM#1Oil
BTM 00117
%
1
Change rate of tensile strength
100°C,70hr,在ASTM#3油中
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,70hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,70hr,inASTM#3Oil
BTM 00117
%
1
Change rate of tensile strength
100°C,168hr,inASTM#1Oil
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,168hr,inASTM#1Oil
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,168hr,inASTM#1Oil
BTM 00117
%
1
Change rate of tensile strength
100%Strain,23°C,336hr,inReferenceFuelA(Isooctane)
BTM 00117
%
-
Change rate of tensile strength
300%Strain,23°C,336hr,inReferenceFuelA(Isooctane)
BTM 00117
%
2
Change rate of tensile strength
23°C,336hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
100%Strain,23°C,336hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
300%Strain,23°C,336hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
23°C,504hr,inReferenceFuelA(Isooctane)
BTM 00117
%
1
Change rate of tensile strength
100%Strain,23°C,504hr,inReferenceFuelA(Isooctane)
BTM 00117
%
7
Change rate of tensile strength
300%Strain,23°C,504hr,inReferenceFuelA(Isooctane)
BTM 00117
%
4
Change rate of tensile strength
23°C,504hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
100%Strain,23°C,504hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,504hr,inASTM#1Oil
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,504hr,inASTM#1Oil
BTM 00117
%
2
Change rate of tensile strength
100°C,504hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,504hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,504hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
100°C,168hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,168hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,168hr,inASTM#3Oil
BTM 00117
%
2
Change rate of tensile strength
100°C,336hr,inASTM#1Oil
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,336hr,inASTM#1Oil
BTM 00117
%
1
Change rate of tensile strength
300%Strain,100°C,336hr,inASTM#1Oil
BTM 00117
%
2
Change rate of tensile strength
100°C,336hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
100%Strain,100°C,336hr,inASTM#3Oil
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,336hr,inASTM#3Oil
BTM 00117
%
1
Change rate of tensile strength
100°C,504hr,inASTM#1Oil
BTM 00117
%
-
Change rate of tensile strength
23°C,168hr,甲醇
ASTMD471
%
-
Change rate of tensile strength
100%Strain,23°C,168hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
300%Strain,23°C,168hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
23°C,336hr,inReferenceFuelA(Isooctane)
ASTMD471
%
1
Change rate of tensile strength
100%Strain,23°C,336hr,inReferenceFuelA(Isooctane)
ASTMD471
%
-
Change rate of tensile strength
300%Strain,23°C,336hr,inReferenceFuelA(Isooctane)
ASTMD471
%
2
Change rate of tensile strength
23°C,336hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
100%Strain,23°C,336hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
300%Strain,23°C,336hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
23°C,504hr,inReferenceFuelA(Isooctane)
ASTMD471
%
1
Change rate of tensile strength
23°C,70hr,inReferenceFuelA(Isooctane)
ASTMD471
%
-
Change rate of tensile strength
100%Strain,23°C,70hr,inReferenceFuelA(Isooctane)
ASTMD471
%
1
Change rate of tensile strength
300%Strain,23°C,70hr,inReferenceFuelA(Isooctane)
ASTMD471
%
1
Change rate of tensile strength
23°C,70hr,甲醇
ASTMD471
%
-
Change rate of tensile strength
100%Strain,23°C,70hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
300%Strain,23°C,70hr,inReferenceFuelC
ASTMD471
%
1
Change rate of tensile strength
23°C,168hr,inReferenceFuelA(Isooctane)
ASTMD471
%
3
Change rate of tensile strength
100%Strain,23°C,168hr,inReferenceFuelA(Isooctane)
ASTMD471
%
0
Change rate of tensile strength
300%Strain,23°C,168hr,inReferenceFuelA(Isooctane)
ASTMD471
%
3
Change rate of tensile strength
300%Strain,23°C,168hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
23°C,336hr,inReferenceFuelA(Isooctane)
BTM 00117
%
1
Change rate of tensile strength
100%Strain,23°C,504hr,inReferenceFuelA(Isooctane)
ASTMD471
%
7
Change rate of tensile strength
300%Strain,23°C,504hr,inReferenceFuelA(Isooctane)
ASTMD471
%
4
Change rate of tensile strength
23°C,504hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
100%Strain,23°C,504hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
300%Strain,23°C,504hr,inReferenceFuelC
ASTMD471
%
-
Change rate of tensile strength
100°C,70hr,在ASTM#1油中
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,70hr,inASTM#1Oil
ASTMD471
%
-
Change rate of tensile strength
300%Strain,100°C,70hr,inASTM#1Oil
ASTMD471
%
1
Change rate of tensile strength
100°C,70hr,在ASTM#3油中
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,70hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
100%Strain,23°C,70hr,inReferenceFuelA(Isooctane)
BTM 00117
%
1
Change rate of tensile strength
300%Strain,23°C,70hr,inReferenceFuelA(Isooctane)
BTM 00117
%
1
Change rate of tensile strength
23°C,70hr,甲醇
BTM 00117
%
-
Change rate of tensile strength
100%Strain,23°C,70hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
300%Strain,23°C,70hr,inReferenceFuelC
BTM 00117
%
1
Change rate of tensile strength
23°C,168hr,inReferenceFuelA(Isooctane)
BTM 00117
%
3
Change rate of tensile strength
100%Strain,23°C,168hr,inReferenceFuelA(Isooctane)
BTM 00117
%
0
Change rate of tensile strength
300%Strain,23°C,168hr,inReferenceFuelA(Isooctane)
BTM 00117
%
3
Change rate of tensile strength
23°C,168hr,甲醇
BTM 00117
%
-
Change rate of tensile strength
100%Strain,23°C,168hr,inReferenceFuelC
BTM 00117
%
-
Change rate of tensile strength
300%Strain,100°C,70hr,inASTM#3Oil
ASTMD471
%
1
Change rate of tensile strength
100°C,168hr,inASTM#1Oil
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,168hr,inASTM#1Oil
ASTMD471
%
-
Change rate of tensile strength
300%Strain,100°C,168hr,inASTM#1Oil
ASTMD471
%
1
Change rate of tensile strength
100°C,168hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,168hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
300%Strain,100°C,168hr,inASTM#3Oil
ASTMD471
%
2
Change rate of tensile strength
100°C,336hr,inASTM#1Oil
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,336hr,inASTM#1Oil
ASTMD471
%
1
Change rate of tensile strength
300%Strain,100°C,336hr,inASTM#1Oil
ASTMD471
%
2
Change rate of tensile strength
100°C,336hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,336hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
300%Strain,100°C,336hr,inASTM#3Oil
ASTMD471
%
1
Change rate of tensile strength
100°C,504hr,inASTM#1Oil
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,504hr,inASTM#1Oil
ASTMD471
%
-
Change rate of tensile strength
300%Strain,100°C,504hr,inASTM#1Oil
ASTMD471
%
2
Change rate of tensile strength
100°C,504hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
100%Strain,100°C,504hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
300%Strain,100°C,504hr,inASTM#3Oil
ASTMD471
%
-
Change rate of tensile strength
23°C,70hr,inReferenceFuelA(Isooctane)
BTM 00117
%
-
Volume change
23°C,70hr,甲醇
ASTMD471
%
4
Volume change
23°C,168hr,inReferenceFuelA
ASTMD471
%
4
Volume change
23°C,168hr,甲醇
ASTMD471
%
4
Volume change
23°C,336hr,inReferenceFuelA
ASTMD471
%
6
Volume change
23°C,336hr,inReferenceFuelC
ASTMD471
%
4
Volume change
23°C,504hr,inReferenceFuelA
ASTMD471
%
7
Volume change
23°C,504hr,inReferenceFuelC
ASTMD471
%
4
Volume change
100°C,70hr,在ASTM#1油中
ASTMD471
%
0
Volume change
100°C,70hr,在ASTM#3油中
ASTMD471
%
1
Volume change
100°C,168hr,inASTM#1Oil
ASTMD471
%
0
Volume change
100°C,504hr,inASTM#3Oil
BTM 00117
%
2
Volume change
23°C,70hr,inReferenceFuelA
ASTMD471
%
3
Volume change
100°C,168hr,inASTM#3Oil
ASTMD471
%
1
Volume change
100°C,336hr,inASTM#1Oil
ASTMD471
%
0
Volume change
100°C,336hr,inASTM#3Oil
ASTMD471
%
2
Volume change
100°C,504hr,inASTM#1Oil
ASTMD471
%
0
Volume change
100°C,504hr,inASTM#3Oil
ASTMD471
%
2
Volume change
23°C,70hr,inReferenceFuelA
BTM 00117
%
3
Volume change
23°C,70hr,甲醇
BTM 00117
%
4
Volume change
23°C,168hr,inReferenceFuelA
BTM 00117
%
4
Volume change
23°C,168hr,甲醇
BTM 00117
%
4
Volume change
23°C,336hr,inReferenceFuelA
BTM 00117
%
6
Volume change
23°C,336hr,inReferenceFuelC
BTM 00117
%
4
Volume change
23°C,504hr,inReferenceFuelA
BTM 00117
%
7
Volume change
23°C,504hr,inReferenceFuelC
BTM 00117
%
4
Volume change
100°C,70hr,在ASTM#1油中
BTM 00117
%
0
Volume change
100°C,70hr,在ASTM#3油中
BTM 00117
%
1
Volume change
100°C,168hr,inASTM#1Oil
BTM 00117
%
0
Volume change
100°C,168hr,inASTM#3Oil
BTM 00117
%
1
Volume change
100°C,336hr,inASTM#1Oil
BTM 00117
%
0
Volume change
100°C,336hr,inASTM#3Oil
BTM 00117
%
2
Volume change
100°C,504hr,inASTM#1Oil
BTM 00117
%
0
Changes in tensile stress during fracture in air
100°C,504hr
ISO216
%
1
Changes in tensile stress during fracture in air
125°C,70hr
ISO216
%
1
Changes in tensile stress during fracture in air
125°C,168hr
ISO216
%
1
Changes in tensile stress during fracture in air
125°C,336hr
ISO216
%
1
Changes in tensile stress during fracture in air
125°C,504hr
ISO216
%
2
Changes in tensile stress during fracture in air
100°C,70hr
ISO216
%
1
Changes in tensile stress during fracture in air
100°C,168hr
ISO216
%
1
Changes in tensile stress during fracture in air
100°C,336hr
ISO216
%
2
elastomer
Test Condition
Test Method
Unit
TPU/COVESTRO GERMANY/985
Basho elasticity
ASTMD2632
%
4
Tensile strength
屈服
ASTMD412
Mpa
3
Tensile stress
50%应变
ISO37
Mpa
4
Tensile stress
50%应变
ASTMD412
Mpa
4
Tensile stress
100%应变
ASTMD412
Mpa
5
Tensile stress
100%应变
ISO37
Mpa
5
Tensile stress
300%应变
ASTMD412
Mpa
9
Tensile stress
300%应变
ISO37
Mpa
9
Tensile stress
屈服
ISO37
Mpa
3
elongation
断裂
ASTMD412
%
5
elongation
断裂
ISO37
%
5
tear strength
ISO34-1
kN/m
8
Tear strength 2
ASTMD624
kN/m
8
Permanent compression deformation
23°C,22hr
ISO815
%
1
Permanent compression deformation
70°C,22hr3
ISO815
%
4
Permanent compression deformation
70°C,22hr
ISO815
%
8
Permanent compression deformation
23°C,22hr3
ASTMD395B
%
1
Permanent compression deformation
23°C,22hr
ASTMD395B
%
1
Permanent compression deformation
70°C,22hr3
ASTMD395B
%
4
Permanent compression deformation
70°C,22hr
ASTMD395B
%
8
Permanent compression deformation
23°C,22hr3
ISO815
%
1
Supplementary Information
Test Condition
Test Method
Unit
TPU/COVESTRO GERMANY/985
CompressiveLoad
10%Deflection
ASTMD575
Mpa
2
CompressiveLoad
15%Deflection
ASTMD575
Mpa
3
CompressiveLoad
2%Deflection
ASTMD575
Mpa
0
CompressiveLoad
20%Deflection
ASTMD575
Mpa
4
CompressiveLoad
25%Deflection
ASTMD575
Mpa
5
CompressiveLoad
5%Deflection
ASTMD575
Mpa
1
CompressiveLoad
50%Deflection
ASTMD575
Mpa
1