Need Help? Contact Us service@plas.com
Get App

PPS RYTON® R-7-120BL CPCHEM USA

167
  • Unit Price:
    $7253 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    142MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Flame retardant High rigidity wear resistant Chemical resistance High temperature resistan Filler: Glass mineral
  • Application Areas:Electronic communication Electronic communication Automotive sector Application in the automo
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageMD:3.20mm0.20%
Modeling ShrinkageTD:3.20mm0.40%
Moisture Absorption23°C,24hrASTMD5700.020%
Density / Specific GravityASTMD7921.99g/cm³
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StrengthASTMD638124Mpa
Flexural StressISO178210Mpa
Compressive StrengthASTMD695265Mpa
Poisson RatioISO5270.36
Tensile StressISO527-2135Mpa
Tensile StrainBreakISO527-20.80%
Tensile ElongationBreakASTMD6380.90%
Flexural ModulusASTMD79019300Mpa
Flexural ModulusISO17819000Mpa
Flexural StrengthASTMD790207Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Deflection Temperature Under Load?1.8MPa,UnannealedASTMD648265°C
Linear thermal expansion coefficientTD:100to200°CASTME8317E-05cm/cm/°C
Linear thermal expansion coefficientTD:导热系数ASTME8310.59W/m/K
Linear thermal expansion coefficientMD:-50to50°CASTME8311.5E-05cm/cm/°C
Linear thermal expansion coefficientMD:100to200°CASTME8311.5E-05cm/cm/°C
Linear thermal expansion coefficientTD:-50to50°CASTME8313E-05cm/cm/°C
UL Temperature RatingUL746B220to240°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
InsulationResistance290°C1E+11ohms
Comparative Tracking IndexCTIUL746250V
Dielectric StrengthASTMD14916KV/mm
Dissipation Factor?25°C,1kHzASTMD1504E-03
Dissipation Factor?25°C,1MHzASTMD1502E-03
Surface ResistivityASTMD2571E+16ohms
Dielectric Constant25°C,1kHzASTMD1504.90
Dielectric Constant25°C,1MHzASTMD1504.90
Arc ResistanceASTMD495185sec
Volume ResistivityASTMD2571E+15ohms·cm
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Notched Izod impact strengthISO18015kJ/m²
Unnotched Izod Impact Strength3.18mmASTMD4812210J/m
Notched Izod Impact Strength3.17mmASTMD25653J/m
Notched Izod Impact StrengthISO180/A6.0kJ/m²
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell HardnessM-SaleASTMD785101
Rockwell HardnessR-SaleASTMD785118
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating1.6mmUL94V-05VA
Oxygen IndexASTMD286361%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.