PPS RYTON® R-4-230BL CPCHEM SINGAPHORE
158
- Unit Price:
- $6653 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 112MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High rigidity Flame retardant Filler: Glass fiber reinf 40% filler by weight 40% filler by weight
- Application Areas:electrical equipment Automotive components Application in the automo
- Color:--
- Grade:Fill level
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | 0.20 | % | |
TD:3.20mm | 0.50 | % | ||
Water absorption rate | 23°C,24hr | ASTMD570 | 0.020 | % |
Density/specific gravity | ASTMD792 | 1.68 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength | ASTMD638 | 165 | Mpa | |
Bending stress | ISO178 | 210 | Mpa | |
compressive strength | ASTMD695 | 275 | Mpa | |
Poisson's ratio | 0.43 | |||
Tensile stress | ISO527-2 | 145 | Mpa | |
Tensile strain | Break | ISO527-2 | 1.1 | % |
elongation | Break | ASTMD638 | 1.2 | % |
Bending modulus | ASTMD790 | 14500 | Mpa | |
ISO178 | 14000 | Mpa | ||
bending strength | ASTMD790 | 221 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 265 | °C |
Linear coefficient of thermal expansion | MD:-50to50°C | ASTME831 | 1.5E-05 | cm/cm/°C |
MD:100to200°C | ASTME831 | 1.5E-05 | cm/cm/°C | |
TD:-50to50°C | ASTME831 | 4E-05 | cm/cm/°C | |
TD:100to200°C | ASTME831 | 8E-05 | cm/cm/°C | |
TD:导热系数 | ASTME831 | 0.31 | W/m/K | |
UL temperature rating | UL746B | 200to220 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
InsulationResistance2 | 90°C | 1E+12 | ohms | |
Compared to the anti leakage trace index | CTI | UL746 | 150 | V |
Dielectric strength | ASTMD149 | 20 | KV/mm | |
Dissipation factor | 25°C,1kHz | ASTMD150 | 2E-03 | |
25°C,1MHz | ASTMD150 | 2E-03 | ||
Surface resistivity | ASTMD257 | 1E+16 | ohms | |
Dielectric constant | 25°C,1kHz | ASTMD150 | 3.90 | |
25°C,1MHz | ASTMD150 | 3.90 | ||
Arc resistance | ASTMD495 | 125 | sec | |
Volume resistivity | ASTMD257 | 1E+16 | ohms·cm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Unscented Izod impact strength | ISO180 | 20 | kJ/m² | |
Cantilever beam without notch impact strength | 3.18mm | ASTMD4812 | 400 | J/m |
Impact strength of cantilever beam gap | 3.17mm | ASTMD256 | 80 | J/m |
ISO180/A | 8.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | M-Sale | ASTMD785 | 104 | |
R-Sale | ASTMD785 | 122 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FlameRating | 1.6mm | UL94 | V-05VA | |
Extreme Oxygen Index | ASTMD2863 | 50 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.