PC/ABS CYCOLAC™ C2950-111 SABIC INNOVATIVE US
249
- Unit Price:
- $2815 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 40MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant High mobility High impact resistance High temperature resistan heat-resisting
- Application Areas:Electrical field Electronic field Household appliances Household appliances Automotive sector
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | 内部方法 | 0.40to0.60 | % |
TD:3.20mm | 内部方法 | 0.40to0.60 | % | |
Water absorption rate | 24hr | ASTMD570 | 0.10 | % |
Equilibrium,23°C | ASTMD570 | 0.40 | % | |
Melt mass flow rate | 260°C/2.16kg | ASTMD1238 | 10 | g/10min |
Density/specific gravity | -- | ASTMD792 | 1.18 | g/cm³ |
--2 | ASTMD792 | 1.22 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength 3 | Yield | ASTMD638 | 62.7 | Mpa |
Bending modulus 4 | 100mmSpan | ASTMD790 | 2650 | Mpa |
Elongation rate 4 | Break | ASTMD638 | 40 | % |
Flexural Strength4 | Yield,100mmSpan | ASTMD790 | 102 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat softening temperature | ASTMD15255 | 113 | °C | |
thermal conductivity | ASTMC177 | 0.20 | W/m/K | |
Linear coefficient of thermal expansion | MD:-30to30°C | ASTMD696 | 7.2E-05 | cm/cm/°C |
TD:-30to30°C | ASTMD696 | 7.2E-05 | cm/cm/°C | |
RTIElec | UL746 | 85.0 | °C | |
Evolution Calendar intelligent importer | UL746 | 85.0 | °C | |
RTIStr | UL746 | 85.0 | °C | |
Hot deformation temperature | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 104 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 90.6 | °C | |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 95.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | ASTMD257 | >1.0E+16 | ohms | |
Dielectric constant | 50Hz | ASTMD150 | 3.00 | |
60Hz | ASTMD150 | 3.00 | ||
100Hz | ASTMD150 | 3.00 | ||
Volume resistivity | ASTMD257 | 1E+17 | ohms·cm | |
Dissipation factor | 50Hz | ASTMD150 | 5E-03 | |
60Hz | ASTMD150 | 5E-03 | ||
100Hz | ASTMD150 | 4.9E-03 | ||
Dielectric strength | 3.20mm,inOil | ASTMD149 | 19 | KV/mm |
Compared to the anti leakage trace index | CTI | UL746 | PLC1 | |
Arc resistance 6 | ASTMD495 | PLC6 | ||
Hot wire ignition | HWI | UL746 | PLC1 | |
High arc combustion index | HAI | UL746 | PLC0 | |
High voltage arc tracing rate | HVTR | UL746 | PLC2 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dart impact equipped with measuring instruments | -30°C,TotalEnergy | ASTMD3763 | 54.2 | J |
23°C,TotalEnergy | ASTMD3763 | 61.0 | J | |
Impact strength of cantilever beam gap | -30°C | ASTMD256 | 160 | J/m |
23°C | ASTMD256 | 530 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Scale | ASTMD785 | 123 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Extreme Oxygen Index | ASTMD2863 | 32 | % | |
UL flame retardant rating | 1.5mm | UL94 | V-0 | |
2.5mm | UL94 | 5VB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.